1.
公开(公告)号:WO2009085757A2
公开(公告)日:2009-07-09
申请号:PCT/US2008/086994
申请日:2008-12-16
Applicant: COOK INCORPORATED , LITHOTECH MEDICAL LTD. , DIAMANT, Valery , KOREN, Dan , LOTKOV, Alexander , SIVOKHA, Vladimir , MEYSNER, Liydmila , GRISHKOV, Viktor , VORONIN, Vladimir
Inventor: DIAMANT, Valery , KOREN, Dan , LOTKOV, Alexander , SIVOKHA, Vladimir , MEYSNER, Liydmila , GRISHKOV, Viktor , VORONIN, Vladimir
CPC classification number: C22C19/03 , A61L29/02 , A61L29/18 , A61L31/022 , A61L31/18 , A61L2400/16 , C22C14/00 , C22F1/10 , C22F1/18
Abstract: A radiopaque alloy based on titanium nickelide and having shape memory and superelastic properties includes, according to one embodiment, at least one radiopaque alloying element selected from the group consisting of gold, platinum, and palladium at a concentration of from about 10 at.% to about 20 at.%, and at least one additional alloying element selected from the group consisting of aluminum, chromium, cobalt, iron, and zirconium, where the additional alloying element has a concentration of from about 0.5 at.% to about 4 at.%. The alloy includes titanium at a concentration of from about 48 at.% to about 52 at.%, and the balance of the alloy is nickel. The radiopaque alloy preferably exhibits superelastic behavior suitable for medical device applications in the human body.
Abstract translation: 根据一个实施方案,基于钛镍合金并具有形状记忆和超弹性的不透射线合金包括至少一种选自金,铂和钯的不透射线的合金元素,浓度为约10原子%至 约20原子%,以及选自铝,铬,钴,铁和锆的至少一种另外的合金元素,其中附加合金元素的浓度为约0.5at。至约4at。 %。 该合金包括浓度为约48原子%至约52原子%的钛,合金的余量为镍。 不透射线的合金优选地表现出适合于人体内医疗器械应用的超弹性行为。
-
2.
公开(公告)号:WO2009085757A3
公开(公告)日:2009-08-27
申请号:PCT/US2008086994
申请日:2008-12-16
Applicant: COOK INC , LITHOTECH MEDICAL LTD , DIAMANT VALERY , KOREN DAN , LOTKOV ALEXANDER , SIVOKHA VLADIMIR , MEYSNER LIYDMILA , GRISHKOV VIKTOR , VORONIN VLADIMIR
Inventor: DIAMANT VALERY , KOREN DAN , LOTKOV ALEXANDER , SIVOKHA VLADIMIR , MEYSNER LIYDMILA , GRISHKOV VIKTOR , VORONIN VLADIMIR
CPC classification number: C22C19/03 , A61L29/02 , A61L29/18 , A61L31/022 , A61L31/18 , A61L2400/16 , C22C14/00 , C22F1/10 , C22F1/18
Abstract: A radiopaque alloy based on titanium nickelide and having shape memory and superelastic properties includes, according to one embodiment, at least one radiopaque alloying element selected from the group consisting of gold, platinum, and palladium at a concentration of from about 10 at.% to about 20 at.%, and at least one additional alloying element selected from the group consisting of aluminum, chromium, cobalt, iron, and zirconium, where the additional alloying element has a concentration of from about 0.5 at.% to about 4 at.%. The alloy includes titanium at a concentration of from about 48 at.% to about 52 at.%, and the balance of the alloy is nickel. The radiopaque alloy preferably exhibits superelastic behavior suitable for medical device applications in the human body.
Abstract translation: 基于镍钛并具有形状记忆和超弹性特性的不透射线合金包括根据一个实施方案的至少一种选自金,铂和钯的不透射线合金元素,浓度为约10原子%至 约20原子%,以及至少一种选自铝,铬,钴,铁和锆的附加合金元素,其中附加合金元素的浓度为约0.5原子%至约4原子% %。 该合金包括浓度为约48原子百分比至约52原子百分比的钛,并且合金的余量为镍。 不透射线的合金优选表现出适用于人体中医疗装置应用的超弹性行为。
-