公开(公告)号:WO2015142311A2
公开(公告)日:2015-09-24
申请号:PCT/US2014/022884
申请日:2014-03-11
Applicant: TAVERNE, Thomas
Inventor: TAVERNE, Thomas
CPC classification number: C04B41/53 , B29C73/26 , E04G23/0203 , Y10T428/20
Abstract: A method for repairing cracked concrete (8) using expansive mortar (13) comprising the steps of installing a saw cut (10) next to an open shrinkage crack (8) and opening the saw cut (10) with expansive mortar (13) to create a wider saw cut (11) and shift half the saw cut (10) toward the open shrinkage crack (8) to close the shrinkage crack (12) tightly. Install a rigid spacer (16) to maintain the width of the control joint. Install adhesive (18) from the top of finished concrete slab (9) into the closed shrinkage crack (12). The surface of the finished concrete slab (9) will receive cosmetic repair (7) to the closed shrinkage crack (12) and let dry before applying sealer. Other embodiments are described as shown.
Abstract translation: 一种使用膨胀砂浆(13)修复裂缝混凝土(8)的方法,包括以下步骤:在开放的收缩裂缝(8)旁边安装锯切口(10),并打开锯切口(10 )用膨胀砂浆(13)形成更宽的锯切(11)并将锯切(10)的一半移向开放收缩裂缝(8)以紧密闭合收缩裂缝(12)。 安装一个刚性垫片(16)以保持控制接头的宽度。 将成品混凝土板(9)顶部的粘合剂(18)装入封闭的收缩裂缝(12)中。 成品混凝土板(9)的表面将接受封闭收缩裂缝(12)的化妆品修补(7),并在涂抹密封胶之前让其干燥。 其他实施例如图所示。 p>
-
公开(公告)号:WO2015142311A8
公开(公告)日:2016-03-10
申请号:PCT/US2014022884
申请日:2014-03-11
Applicant: TAVERNE THOMAS
Inventor: TAVERNE THOMAS
CPC classification number: C04B41/53 , B29C73/26 , E04G23/0203 , Y10T428/20
Abstract: A method for repairing cracked concrete (8) using expansive mortar (13) comprising the steps of installing a saw cut (10) next to an open shrinkage crack (8) and opening the saw cut (10) with expansive mortar (13) to create a wider saw cut (11) and shift half the saw cut (10) toward the open shrinkage crack (8) to close the shrinkage crack (12) tightly. Install a rigid spacer (16) to maintain the width of the control joint. Install adhesive (18) from the top of finished concrete slab (9) into the closed shrinkage crack (12). The surface of the finished concrete slab (9) will receive cosmetic repair (7) to the closed shrinkage crack (12) and let dry before applying sealer. Other embodiments are described as shown.
Abstract translation: 一种使用膨胀砂浆(13)修复裂纹混凝土(8)的方法,包括以下步骤:在开放收缩裂缝(8)旁边安装锯切(10)并用膨胀砂浆(13)将锯切(10)打开至 产生更宽的锯切(11),并将锯切(10)的一半朝向开放的收缩裂缝(8)移动,以紧密地收缩收缩裂缝(12)。 安装一个刚性垫片(16)以保持控制接头的宽度。 将成品混凝土板(9)顶部的粘合剂(18)安装到封闭的收缩裂缝(12)中。 完成的混凝土板(9)的表面将接收封闭收缩裂缝(12)的化妆品修复(7),并在施加密封剂之前进行干燥。 其他实施例如图所示进行描述。
-
公开(公告)号:WO2015142311A3
公开(公告)日:2015-11-12
申请号:PCT/US2014022884
申请日:2014-03-11
Applicant: TAVERNE THOMAS
Inventor: TAVERNE THOMAS
CPC classification number: C04B41/53 , B29C73/26 , E04G23/0203 , Y10T428/20
Abstract: A method for repairing cracked concrete (8) using expansive mortar (13) comprising the steps of installing a saw cut (10) next to an open shrinkage crack (8) and opening the saw cut (10) with expansive mortar (13) to create a wider saw cut (11) and shift half the saw cut (10) toward the open shrinkage crack (8) to close the shrinkage crack (12) tightly. Install a rigid spacer (16) to maintain the width of the control joint. Install adhesive (18) from the top of finished concrete slab (9) into the closed shrinkage crack (12). The surface of the finished concrete slab (9) will receive cosmetic repair (7) to the closed shrinkage crack (12) and let dry before applying sealer. Other embodiments are described as shown.
Abstract translation: 一种使用膨胀砂浆(13)修补裂缝混凝土(8)的方法,包括以下步骤:在打开的收缩裂缝(8)旁边安装锯切口(10),并用膨胀砂浆(13)打开锯切口(10) 创建更宽的锯切(11)并将锯切(10)的一半移向开放收缩裂缝(8)以紧密闭合收缩裂缝(12)。 安装一个刚性垫片(16)以保持控制接头的宽度。 将成品混凝土板(9)顶部的粘合剂(18)装入封闭的收缩裂缝(12)中。 成品混凝土板(9)的表面将接受封闭收缩裂缝(12)的化妆品修补(7),并在涂抹密封胶之前让其干燥。 其他实施例如图所示进行描述。
-
公开(公告)号:WO2015142311A4
公开(公告)日:2015-12-10
申请号:PCT/US2014022884
申请日:2014-03-11
Applicant: TAVERNE THOMAS
Inventor: TAVERNE THOMAS
CPC classification number: C04B41/53 , B29C73/26 , E04G23/0203 , Y10T428/20
Abstract: A method for repairing cracked concrete (8) using expansive mortar (13) comprising the steps of installing a saw cut (10) next to an open shrinkage crack (8) and opening the saw cut (10) with expansive mortar (13) to create a wider saw cut (11) and shift half the saw cut (10) toward the open shrinkage crack (8) to close the shrinkage crack (12) tightly. Install a rigid spacer (16) to maintain the width of the control joint. Install adhesive (18) from the top of finished concrete slab (9) into the closed shrinkage crack (12). The surface of the finished concrete slab (9) will receive cosmetic repair (7) to the closed shrinkage crack (12) and let dry before applying sealer. Other embodiments are described as shown.
Abstract translation: 一种使用膨胀砂浆(13)修复裂纹混凝土(8)的方法,包括以下步骤:在开放收缩裂缝(8)旁边安装锯切(10)并用膨胀砂浆(13)打开锯切(10)至 产生更宽的锯切(11),并将锯切(10)的一半朝向开放的收缩裂缝(8)移动,以紧密地收缩收缩裂缝(12)。 安装一个刚性垫片(16)以保持控制接头的宽度。 将成品混凝土板(9)顶部的粘合剂(18)安装到封闭的收缩裂缝(12)中。 完成的混凝土板(9)的表面将接收封闭收缩裂缝(12)的化妆品修复(7),并在施加密封剂之前进行干燥。 其他实施例如图所示进行描述。
-
-
-