LABELED CONTAINERS, METHODS AND DEVICES FOR MAKING SAME
    1.
    发明申请
    LABELED CONTAINERS, METHODS AND DEVICES FOR MAKING SAME 审中-公开
    标签容器,用于制造该标签的方法和设备

    公开(公告)号:WO2008022180A2

    公开(公告)日:2008-02-21

    申请号:PCT/US2007/075980

    申请日:2007-08-15

    Abstract: A labeled expanded resin container that includes pre-expanded resin beads molded in a shape having a sidewall with an outer surface and a base; and a label formed from a label material capable of maintaining an electrostatic charge disposed over at least a portion of the outer surface of the sidewall of the container. The container has a rim strength that is at least 50% greater than the rim strength of a container that does not contain a label, where the containers are otherwise made using the same equipment. After a liquid at 50°F (10°C) is placed in the container and the container is exposed to conditions of 86°F (30°C) and 60% relative humidity for 30 minutes, less than 2 ml of moisture condenses on the outer surface of the container.

    Abstract translation: 标记的发泡树脂容器,其包括预成型的树脂珠粒,该预成型的树脂珠粒以具有外表面和底部的侧壁的形状模制而成; 以及由能够维持静电荷的标签材料形成的标签,该标签布置在容器的侧壁的外表面的至少一部分上。 容器的边缘强度比不包含标签的容器的边缘强度大至少50%,其中容器另外使用相同的设备制造。 在将50°F(10℃)的液体置于容器中并将容器暴露于86°F(30℃)和60%相对湿度的条件下30分钟后,少于2ml的水分在 容器的外表面。

    LABELED CONTAINERS, METHODS AND DEVICES FOR MAKING SAME
    2.
    发明申请
    LABELED CONTAINERS, METHODS AND DEVICES FOR MAKING SAME 审中-公开
    标签容器,制造方法和装置

    公开(公告)号:WO2008022180A3

    公开(公告)日:2008-10-02

    申请号:PCT/US2007075980

    申请日:2007-08-15

    Abstract: A labeled expanded resin container that includes pre-expanded resin beads molded in a shape having a sidewall with an outer surface and a base; and a label formed from a label material capable of maintaining an electrostatic charge disposed over at least a portion of the outer surface of the sidewall of the container. The container has a rim strength that is at least 50% greater than the rim strength of a container that does not contain a label, where the containers are otherwise made using the same equipment. After a liquid at 50°F (10°C) is placed in the container and the container is exposed to conditions of 86°F (30°C) and 60% relative humidity for 30 minutes, less than 2 ml of moisture condenses on the outer surface of the container.

    Abstract translation: 一种标记的膨胀树脂容器,其包括模制成具有外表面和底部的侧壁的形状的预发泡树脂珠粒; 以及由能够保持静电电荷的标签材料形成的标签,其设置在容器的侧壁的至少一部分外表面上。 容器具有的边缘强度比不含标签的容器的边缘强度大至少50%,其中容器使用相同的设备制造。 将50°F(10°C)的液体置于容器中,容器暴露于86°F(30°C)和60%相对湿度条件下30分钟,少于2ml的湿气会冷凝 容器的外表面。