A WELDING METHOD
    1.
    发明申请
    A WELDING METHOD 审中-公开

    公开(公告)号:WO2023002269A1

    公开(公告)日:2023-01-26

    申请号:PCT/IB2022/055737

    申请日:2022-06-21

    Applicant: ARCELORMITTAL

    Abstract: The invention relates to a welding method for the manufacture of an assembly of at least two steel substrates spot welded together through at least one spot welded joint, comprising: A. The provision of said substrates (3, 3') wherein a first one is a press hardened steel part obtained by press hardening of a steel sheet coated with an aluminium based coating, B. The application of a spot-welding cycle with a spot-welding machine, comprising welding electrodes (1,T) and a spot-welding power source (2) applying a current, through said substrates, said cycle (21) consisting of: - at least three pulsations (22, 32, 42), each having the same maximum pulsation current (Cp) applied through said substrates, each pulsation duration p being identical and set from 20 to 60 ms, - each pulsation being followed by the same cooling time c set from 30 to 50 ms, wherein the welding parameter Wp value is at least 0.8, Wp being defined as Wp = (t x c)/p t being the average thickness of the substrate in mm, c being the cooling time in ms, p being the pulsation duration in ms.

    A WELDING METHOD
    2.
    发明申请
    A WELDING METHOD 审中-公开

    公开(公告)号:WO2023002239A1

    公开(公告)日:2023-01-26

    申请号:PCT/IB2021/056661

    申请日:2021-07-23

    Applicant: ARCELORMITTAL

    Abstract: The invention relates to a welding method for the manufacture of an assembly of at least two steel substrates spot welded together through at least one spot welded joint, comprising: A. The provision of said substrates (3, 3') wherein a first one is a press hardened steel part obtained by press hardening of a steel sheet coated with an aluminium based coating, B. The application of a spot-welding cycle with a spot-welding machine, comprising welding electrodes (1,1') and a spot-welding power source (2) applying a current, through said substrates, said cycle (21) consisting of: - at least three pulsations (22, 32, 42), each having the same maximum pulsation current (Cp) applied through said substrates, each pulsation duration p being identical and set from 20 to 60 ms, - each pulsation being followed by the same cooling time c set from 30 to 50 ms, wherein the welding parameter Wp value is at least 0.8, Wp being defined as Wp = (t x c)/p t being the average thickness of the substrate in mm, c being the cooling time in ms, p being the pulsation duration in ms.

Patent Agency Ranking