Abstract:
A process to make a friable bale, and a friable bale formed from the same, wherein the friable bale is formed from a composition comprising coated polymer particles, which comprise polymer particles formed from a polymer composition comprising an olefin-based polymer, and a coating formed from a coating composition comprising an aqueous metal acid dispersion, and an aqueous polysiloxane emulsion, and wherein the friable bale has a compression force ≤ 1.00 MPa.
Abstract:
The process for making extra high voltage cable insulation is improved by using a composition comprising in weight percent based on the weight of the composition: (A) 95 to 99.9% of an ethylene-based polymer; (B) 0.2 to 2.5% peroxide; (C) 0.01 to 0.5% of a sulfur-containing first antioxidant having at least one -S(CH 2 )2CO 2 R group, wherein R is a C6 to C20 alkyl; (D) 0.001 to 0.009%) of a phosphorus-containing second antioxidant that does not contain a -S(CH 2 ) 2 C0 2 R group, wherein R is a C6 to C20 alkyl; (E) Optionally, an organic nitrogenous base; and (F) Optionally, a phenolic third antioxidant that does not contain a -S(CH 2 ) 2 C0 2 R group, wherein R is a C6 to C20 alkyl.
Abstract:
The process for making extra high voltage cable insulation is improved by using a composition comprising in weight percent based on the weight of the composition: (A) 95 to 99.9% of an ethylene-based polymer; (B) 0.2 to 2.5% peroxide; (C) 0.01 to 0.5% of a sulfur-containing first antioxidant having at least one -S(CH 2 ) 2 C0 2 R group, wherein R is C6 to C20 alkyl; (D) 0.001 to 0.009%) of a sulfur-containing second antioxidant that does not contain a -S(CH 2 ) 2 C0 2 R group, wherein R is a C6 to C20 alkyl; (E) Optionally, an organic nitrogenous base; and (F) Optionally, a phenolic third antioxidant that does not contain a -S(CH 2 ) 2 C0 2 R group, wherein R is a C6 to C20 alkyl.