1.
公开(公告)号:WO2022071992A1
公开(公告)日:2022-04-07
申请号:PCT/US2021/027966
申请日:2021-04-19
Applicant: ICON TECHNOLOGY, INC.
Inventor: MARKANDEYA, Ananya , GALVEZ MORENO, Daniel , LEY HERNANDEZ, Aida Margarita , KUPWADE-PATIL, Kunal , LE ROUX, Alexander
IPC: B28B1/00 , B29C64/106 , B28B17/00 , B33Y10/00
Abstract: A 3D printable clay-based mortar cementitious ink includes a blend of commercially available Portland cement, calcium carbonate, sand, and calcined clay. The calcined clay is produced from the calcination of clay having a high kaolinite content of greater than about 60%. The clay is calcined at a temperature of between about 600°C and about 800°C, preferably between about 650°C and about 850°C, for a period of one to two hours. In a preferred embodiment, a ratio of calcined clay to Portland cement is about 0.148, a ratio of calcium carbonate to Portland cement is about 0.333, and a ratio of sand to Portland cement is approximately about 3.0. The ratio of water to powder (clay, cement, calcium carbonate, and sand) may range between 0.39 and 0.40.