Abstract:
A highly purified diatomite composition may indude greater than or equal to 90% silica, from about 0.5% to about 5% of a calcium-containing compound, and less than or equal to about 2% total of aluminum-containing oxides and iron-containing oxides. A method of making a highly purified diatomite composition may include providing a diatomite comprising at least 5% of a calcium-containing compound, calcining the diatomite, and acid washing the calcined diatomite. The calcined, acid-washed diatomite may include less than or equal to about 1 % total of extractable aluminum-containing oxides and iron-containing oxides, and less than or equal to about 5% of the calcium-containing compound. The acid washing may include an acid selected from the group consisting of sulfuric acid (Η 2 SO 4 ), hydrochloric acid (HCI), and nitric acid (HNO 3 ). The method may not include a flotation step.
Abstract:
A method of producing a polymer foam may include providing a polymer composition, introducing an alkaline earth metal silicate into the polymer composition, and foaming the polymer composition using a gas to form a polymer foam. A method of producing a polymer-matrix may include providing a polymer composition, nucleating the polymer composition with an alkaline earth metal silicate, and using a blowing agent to form a polymer foam from the polymer composition. The alkaline earth metal silicate may facilitate nucleation of the cells in the polymer foam. A polymer foam composition may include a polymer-based foam matrix and an alkaline earth metal silicate within a cell of the polymer-based foam matrix.
Abstract:
Disclosed herein are methods of preventing or reducing scale formation or corrosion by combining at least one scale-forming fluid comprising at least one scaling compound with at least one anti-scale material chosen from at least one scale-adsorbent agent. The methods may reduce or prevent the formation of scale on surfaces of liquid-related process equipment, such as boilers and heat exchangers.
Abstract:
A method for calcining diatomaceous earth may include adding at least one lattice interfering agent to the diatomaceous earth to form a composite material. The method may further include heating the composite material at a temperature of at least about 800°C for at least about 15 minutes to form an at least partially calcined composite material. The at least one lattice interfering agent may include at least one cation of at least one of aluminum and titanium. A diatomaceous earth product may include the at least partially calcined composite material formed from the above- noted method for calcining diatomaceous earth. A filter aid may include the diatomaceous earth product.
Abstract:
A method for removing 4-rnethylimidazole (4-MEI) from solution may include contacting an alkaline earth metal silicate with a solution containing 4-MEI and adsorbing at least some of the 4-MEI using the alkaline earth metal silicate. The method may further include removing at least some of the alkaline earth metal silicate having the adsorbed 4-MEI from the solution. The alkaline earth metal silicate may include magnesium silicate or calcium silicate. A method for removing 4-MEI from solution may include contacting an adsorbent clay material with a solution containing 4-MEI and adsorbing at least some of the 4-MEI using the adsorbent clay material. The method may further include removing at least some of the adsorbent clay material having the adsorbed 4-MEI from the solution. The adsorbent clay material may include smectite, bentonite, or an activated or un-activated AOCS clay material.