1.
公开(公告)号:WO1984000536A1
公开(公告)日:1984-02-16
申请号:PCT/SU1982000024
申请日:1982-07-30
Inventor: MOSKOVSKY KHIMIKO-TEKHNOLOGICHESKY INSTITUT IMENI , PAVLUSHKIN, Nikolai Mikheevich , KAVANOV, Nikolai Pavlovich , SARKISOV, Pavel Dzhibraelovich , SCHUKIN, Vitaly Sergeevich , ORLOVA, Ljudmila, Alexeevna , PESHKOV, Vladimir, Mikhailovich , BORISOVA, Olga Nikolaevna , PODLESNAYA, Galina Vladlenovna , KHAIRETDINOVA, Leilya Safovna
IPC: C03C03/22
CPC classification number: C03C10/0063 , C03C10/0036 , C03C10/0045 , C03C10/16
Abstract: The glass crystalline material bears a granitoid semblance and in general consists of beta -wollastonite crystals, being in the shape of spherulites, at the following ratio in % by mass: SiO2 55.0-60.0, Al2O3 6.0-9.0, CaO 17.0-25.0, MgO 3.0-10.0, K2O 5.0-7.0, Na2O 1.0-2.0, F 1.0-2.5; The method for obtaining the material provides for moulding the glass from a melt, which melt contains SiO2, Al2O3, CaO, MgO, Na2O, K2O, F , its cooling down to the temperature which is 30-50 C lower than the temperature of the glass-transition, and performing the thermal treatment of the glass untill achieving its transformation into said glass crystalline material.
Abstract translation: 玻璃结晶材料具有花岗岩外观,通常由球晶形状的β-硅灰石晶体组成,按以下的质量%:SiO 2 55.0-60.0,Al 2 O 3 6.0-9.0,CaO 17.0-25.0,MgO 3.0-10.0,K2O 5.0-7.0,Na2O 1.0-2.0,F - 1.0-2.5; 获得该材料的方法提供了从熔体中熔化的玻璃,该熔体含有SiO 2,Al 2 O 3,CaO,MgO,Na 2 O,K 2 O,F 2,其冷却至30-50℃ 低于玻璃化转变的温度,并进行玻璃的热处理,直到实现其转变为所述玻璃结晶材料。