KAOLIN CLAY SLURRIES HAVING REDUCED VISCOSITIES AND PROCESS FOR THE MANUFACTURE THEREOF
    1.
    发明申请
    KAOLIN CLAY SLURRIES HAVING REDUCED VISCOSITIES AND PROCESS FOR THE MANUFACTURE THEREOF 审中-公开
    具有降低粘度的KAOLIN粘土浆和其制造方法

    公开(公告)号:WO1997001390A1

    公开(公告)日:1997-01-16

    申请号:PCT/US1996010828

    申请日:1996-06-25

    CPC classification number: C09C1/42 C01P2006/22

    Abstract: A kaolin clay slurry having a reduced viscosity is manufactured by a process which comprises the sequential steps of mechanically working an undispersed crude kaolin clay material having a solids content of at least about 65 percent, by weight, under conditions which insure that the kaolin clay material will be subjected to an energy level of at least 10 horsepower-hours per ton of dry kaolin clay material and then subjecting the mechanically worked kaolin clay material to centrifugation to substantially remove any particles having a diameter less than about 0.2 microns.

    Abstract translation: 通过包括以下步骤的方法制造具有降低的粘度的高岭土粘土浆料,该方法包括在确保高岭土粘土材料的条件下机械加工固体含量为至少约65重量%的未分散的粗高岭土粘土材料的顺序步骤 将经受每吨干燥高岭土粘土材料至少10马力 - 小时的能级,然后将机械加工的高岭土材料进行离心以基本上除去直径小于约0.2微米的任何颗粒。

Patent Agency Ranking