公开(公告)号:WO2013045551A8
公开(公告)日:2014-04-10
申请号:PCT/EP2012069086
申请日:2012-09-27
Applicant: TITAN WOOD LTD
Abstract: Disclosed are panels of medium density fibreboard (MDF). The panels comprise wood fibres, the largest dimension of which is 7 mm or below, pressed together with an adhesive. The panels are of a large and thin type, having an aspect ratio of at least 100 and a surface area of at least 1 m2. Typical problems associated with such large and thin panels, e.g. warping behaviour, are addressed by employing wood fibres are made of acetylated wood.
Abstract translation: 公开了中密度纤维板(MDF)的面板。 面板包括木质纤维,其最大尺寸为7毫米或更小,用粘合剂压在一起。 这些面板是大而薄的,具有至少100的纵横比和至少1m 2的表面积。 与这种大型和薄型板相关的典型问题,例如 翘曲行为,通过采用木纤维来解决,由乙酰化木制成。
-
公开(公告)号:WO2013139937A8
公开(公告)日:2014-11-06
申请号:PCT/EP2013055983
申请日:2013-03-21
Applicant: TITAN WOOD LTD
Inventor: POL BERNARDUS JOZEF MARIA , VAN DOMMELE STEFAN , BUSSEMAKER PAUL , PAINTER BENJAMIN , DE WIT GERRIT ARIE , KAPPEN THEODORUS GERARDUS MARINUS MARIA
CPC classification number: C08H8/00 , B01J8/10 , B05D3/0209 , B05D3/04 , B05D7/10 , B27K3/08 , B27K3/10 , B27K3/346 , C08L97/02
Abstract: The invention is directed to a process for the continuous acetylation of wood elements. The process particularly combines a batchwise impregnation step, with a continuous reaction step. In order to realize this, a collection step is built-in, so as to allow batches of impregnated wood elements to be fed into a reactor in a continuous manner. Very high acetylation contents can be obtained, at a level that had not been achievable before in a continuous and non-catalyzed acetylation process.
Abstract translation: 本发明涉及木质元素的连续乙酰化的方法。 该方法特别地结合了分批浸渍步骤和连续反应步骤。 为了实现这一点,内置了收集步骤,以便允许批量的浸渍木质元件以连续的方式进料到反应器中。 可以获得非常高的乙酰化含量,其水平在连续和非催化乙酰化过程之前尚未实现。
-
公开(公告)号:WO2013139937A3
公开(公告)日:2013-11-14
申请号:PCT/EP2013055983
申请日:2013-03-21
Applicant: TITAN WOOD LTD
Inventor: POL BERNARDUS JOZEF MARIA , VAN DOMMELE STEFAN , BUSSEMAKER PAUL , PAINTER BENJAMIN , DE WIT GERRIT ARIE , KAPPEN THEODORUS GERARDUS MARINUS MARIA
CPC classification number: C08H8/00 , B01J8/10 , B05D3/0209 , B05D3/04 , B05D7/10 , B27K3/08 , B27K3/10 , B27K3/346 , C08L97/02
Abstract: The invention is directed to a process for the continuous acetylation of wood elements. The process particularly combines a batchwise impregnation step, with a continuous reaction step. In order to realize this, a collection step is built-in, so as to allow batches of impregnated wood elements to be fed into a reactor in a continuous manner. Very high acetylation contents can be obtained, at a level that had not been achievable before in a continuous and non-catalyzed acetylation process.
Abstract translation: 本发明涉及木质元素的连续乙酰化的方法。 该方法特别地结合了分批浸渍步骤和连续反应步骤。 为了实现这一点,内置了收集步骤,以便允许批量的浸渍木质元件以连续的方式进料到反应器中。 可以获得非常高的乙酰化含量,其水平在连续和非催化乙酰化过程之前尚未实现。
-
-