Abstract:
The present invention describes a corrosion control electrolyte coating system and methods to protect steel surface above ground and off-shore facilities from rusting and corrosion, wherein the steel surface is exposed to the atmospheric environment and coated by a transparent, ionically conductive, and dried layer or film. The system mainly made of four elements i.e. an anode, an electrolyte connected to the anode by an conductive adhesive, a power source e.g. DC power source, and a metal structure to be protected from corrosion, or rusting due to environment or atmospheric factors. The electrolyte used in the present system further comprises a highly ionically conductive & hydrophilic fluoropolymer resin having anti-cracking properties. The coating liquid can be applied easily onto the metal structure above the ground just like ordinary paints and functions well as an electrolyte of the cathodic protection. The coating liquid applied on the metal surface leads to the realization of the cathodic protection of the ground.
Abstract:
A roofing material composition and a method of applying that roofing material composition using specific angles to deflect infra-red rays and provide aesthetically nice finish is disclosed. The first coat of the roofing material is light in color and the second color may be a light or a dark color. The rough surface is prepared using specific filler, resin and paint to deflect infra-red rays and reduce heating inside a building.
Abstract:
The present invention is related to a thermo-shielding window coating composition having improved thermo-shielding and weathering resistant properties when applied to glass surfaces. The composition is made by first mixing an infrared absorbing pigment in amount of up to 5 wt.% with first dosage of an aqueous or alcoholic sulfonate group grafted fluoropolymer resin in amount of up to 10 wt.%, and water in amount of up to 10 wt.% to obtain a mixer, then dispersing the mixer by a disperser, and simultaneously adding second dosage of the sulfonate group grafted fluoropolymer resin in amount up to 90 wt.% to the above mixer until homogenous solution is obtained, wherein the weight % is calculated based on the total weight of the coating composition.