Invention Grant
- Patent Title: Lithium-ion-conductive ceramic material, lithium-ion-conductive ceramic sintered body, and lithium battery
-
Application No.: US15858362Application Date: 2017-12-29
-
Publication No.: US11011776B2Publication Date: 2021-05-18
- Inventor: Yuki Takeuchi , Hirofumi Ando , Daisuke Shishihara , Hidetoshi Mizutani
- Applicant: NGK SPARK PLUG CO., LTD.
- Applicant Address: JP Nagoya
- Assignee: NGK SPARK PLUG CO., LTD.
- Current Assignee: NGK SPARK PLUG CO., LTD.
- Current Assignee Address: JP Nagoya
- Agency: Stites & Harbison, PLLC
- Agent Jeffrey A. Haeberlin; Terry L. Wright
- Main IPC: H01M10/0562
- IPC: H01M10/0562 ; C04B35/48 ; C04B35/626 ; C04B35/64 ; H01M10/0525 ; C04B35/486 ; H01M4/62 ; H01M10/052

Abstract:
[OBJECTS]
An object of the present invention is to provide a lithium-ion-conductive ceramic material having a target ion conductivity, while suppressing production cost. Another object is to provide a high-performance lithium battery, while suppressing production cost, by virtue of having the lithium-ion-conductive ceramic material.
The lithium-ion-conductive ceramic material contains Li, La, and Zr, as well as at least one of Mg and A (wherein A represents at least one element selected from the group consisting of Ca, Sr, and Ba) and which has a garnet-type crystal structure, wherein the elements contained in the ceramic material satisfy the following mole ratio conditions (1) to (3): (1) 1.33≤Li/(La+A)≤3; (2) 0
An object of the present invention is to provide a lithium-ion-conductive ceramic material having a target ion conductivity, while suppressing production cost. Another object is to provide a high-performance lithium battery, while suppressing production cost, by virtue of having the lithium-ion-conductive ceramic material.
The lithium-ion-conductive ceramic material contains Li, La, and Zr, as well as at least one of Mg and A (wherein A represents at least one element selected from the group consisting of Ca, Sr, and Ba) and which has a garnet-type crystal structure, wherein the elements contained in the ceramic material satisfy the following mole ratio conditions (1) to (3): (1) 1.33≤Li/(La+A)≤3; (2) 0