Invention Grant
- Patent Title: Method for producing transparent conducting film
-
Application No.: US17763067Application Date: 2020-05-29
-
Publication No.: US11538603B2Publication Date: 2022-12-27
- Inventor: Shigeru Yamaki , Shuhei Yoneda
- Applicant: SHOWA DENKO K.K.
- Applicant Address: JP Tokyo
- Assignee: SHOWA DENKO K.K.
- Current Assignee: SHOWA DENKO K.K.
- Current Assignee Address: JP Tokyo
- Agency: Sughrue Mion, PLLC
- Priority: JPJP2019-238102 20191227
- International Application: PCT/JP2020/021400 WO 20200529
- International Announcement: WO2021/131099 WO 20210701
- Main IPC: B32B37/14
- IPC: B32B37/14 ; B82Y40/00 ; H01B1/22 ; H01B5/14 ; B82Y30/00

Abstract:
Provided is a transparent conducting film containing metal nanowires, the conducting film having a preferable optical property, electrical property, and having almost no in-plane resistance anisotropy.
A method for producing a transparent conducting film provided with a conducting layer containing a metal nanowire and a binder resin, comprising steps of: preparing a coating liquid containing the metal nanowire and the binder resin, and coating the coating liquid on one main face of a transparent substrate, the coating step being performed by a bar-coater with a bar which has a bar surface constituted by a material having a friction coefficient of 0.05 to 0.45, wherein when the coating liquid is coated on one main face of the transparent substrate by the bar, a relative moving velocity (coating velocity) V (mm/sec) of the transparent substrate relative to the bar satisfies 2000≥V≥350, a groove formed on the bar has a pitch (P) and a depth (H) which satisfy a ratio P/H of 9 to 30, and on the bar surface, the groove is formed to be inclined in a way so that an angle between the longitudinal direction of the bar and a direction that the groove is formed is in a range of 60° to 88°.
A method for producing a transparent conducting film provided with a conducting layer containing a metal nanowire and a binder resin, comprising steps of: preparing a coating liquid containing the metal nanowire and the binder resin, and coating the coating liquid on one main face of a transparent substrate, the coating step being performed by a bar-coater with a bar which has a bar surface constituted by a material having a friction coefficient of 0.05 to 0.45, wherein when the coating liquid is coated on one main face of the transparent substrate by the bar, a relative moving velocity (coating velocity) V (mm/sec) of the transparent substrate relative to the bar satisfies 2000≥V≥350, a groove formed on the bar has a pitch (P) and a depth (H) which satisfy a ratio P/H of 9 to 30, and on the bar surface, the groove is formed to be inclined in a way so that an angle between the longitudinal direction of the bar and a direction that the groove is formed is in a range of 60° to 88°.