发明申请
- 专利标题: Boron carbide based sintered compact and method for preparation thereof
- 专利标题(中): 碳化硼基烧结体及其制备方法
-
申请号: US11477433申请日: 2006-06-30
-
公开(公告)号: US20060247120A1公开(公告)日: 2006-11-02
- 发明人: Kiyoshi Hirao , Shuji Sakaguchi , Yukihiko Yamauchi , Shuzo Kanzaki , Suzuya Yamada
- 申请人: Kiyoshi Hirao , Shuji Sakaguchi , Yukihiko Yamauchi , Shuzo Kanzaki , Suzuya Yamada
- 申请人地址: JP Tokyo JP Tokyo
- 专利权人: Nat'l Inst. of Advanced Ind. Science and Tech.,Denki Kagaku Kogyo Kabushiki Kaisha
- 当前专利权人: Nat'l Inst. of Advanced Ind. Science and Tech.,Denki Kagaku Kogyo Kabushiki Kaisha
- 当前专利权人地址: JP Tokyo JP Tokyo
- 优先权: JP2001-341205 20011106; JP2002-131272 20020507
- 主分类号: C04B35/563
- IPC分类号: C04B35/563
摘要:
A boron carbide based sintered body having a four-point flexural strength of at least 400 MPa and a fracture toughness of at least 2.8 MPa·m1/2, which has the following two preferred embodiments. (1) A boron carbide-titanium diboride sintered body obtained by sintering a mixed powder of a B4C powder, a TiO2 powder and a C powder while reacting them under a pressurized condition and comprising from 95 to 70 mol % of boron carbide and from 5 to 30 mol % of titanium diboride, wherein the boron carbide has a maximum particle diameter of at most 5 μm. (2) A boron carbide-chromium diboride sintered body containing from 10 to 25 mol % of CrB2 in B4C, wherein the sintered body has a relative density of at least 90%, boron carbide particles in the sintered body have a maximum particle diameter of at most 100 μm, and the abundance ratio (area ratio) of boron carbide particles of from 10 to 100 μm to boron carbide particles having a particle diameter of at most 5 μm, is from 0.02 to 0.6.