- Patent Title: Process for the preparation of LiFePO4-carbon composites
- Patent Title (中): 制备LiFePO4-碳复合材料的方法
-
Application No.: US13379048Application Date: 2010-06-23
-
Publication No.: US09209461B2Publication Date: 2015-12-08
- Inventor: Simon Schroedle , Hartmut Hibst , Brian Roberts , Kirill Bramnik , Jordan Keith Lampert
- Applicant: Simon Schroedle , Hartmut Hibst , Brian Roberts , Kirill Bramnik , Jordan Keith Lampert
- Applicant Address: DE Ludwigshafen
- Assignee: BASF SE
- Current Assignee: BASF SE
- Current Assignee Address: DE Ludwigshafen
- Agency: Oblon, McClelland, Maier & Neustadt, L.L.P.
- International Application: PCT/EP2010/058868 WO 20100623
- International Announcement: WO2010/149681 WO 20101229
- Main IPC: H01B1/24
- IPC: H01B1/24 ; H01M4/525 ; H01M4/58 ; C01B25/45 ; C01B25/455 ; H01M4/131 ; H01M4/1315 ; H01M4/133 ; H01M4/485 ; H01M4/505 ; H01M4/583 ; H01M10/0525

Abstract:
The present invention relates to a process for the preparation of particles comprising at least one compound according to general formula (I) M1aM2bM3cOoNnFf (I) wherein M1, M2, M3 O, N, F, a, b, c, o, n and f have the following meanings: M1 at least one alkaline metal, M2 at least one transition metal in oxidation state +2, M3 at least one non-metal chosen form S, Se, P, As, Si, Ge and/or B, O oxygen, N nitrogen, F fluorine, a 0.8-4.2, b 0.8-1.9, c 0.8-2.2, o 1.0-8.4, n 0-2.0 and f 0-2.0, wherein a, b, c, o, n and f are chosen to ensure electroneutrality of the compound according to general formula (I), and carbon, comprising at least the following steps: (A) providing an essentially aqueous mixture comprising at least one compound comprising M1, at least one compound comprising M2 having at least partially an oxidation state higher than +2, optionally at least one compound comprising M3, at least one compound comprising N, if present, and/or at least one compound comprising F, if present, at least one polysaccharide comprising glucose having a molecular weight M of at least 50000 g/mol as carbon precursor and at least one reducing agent, (B) drying the mixture provided in step (A), in order to obtain a solid particle and (C) calcining the solid particle obtained from step (B) at a temperature of 300 to 950° C.