Invention Grant
- Patent Title: Process for producing porous sintered aluminum, and porous sintered aluminum
- Patent Title (中): 生产多孔烧结铝的方法和多孔烧结铝
-
Application No.: US13260962Application Date: 2010-03-30
-
Publication No.: US09242297B2Publication Date: 2016-01-26
- Inventor: Koji Hoshino , Ji-bin Yang , Kenji Orito , Shinichi Ohmori
- Applicant: Koji Hoshino , Ji-bin Yang , Kenji Orito , Shinichi Ohmori
- Applicant Address: JP Tokyo
- Assignee: MITSUBISHI MATERIALS CORPORATION
- Current Assignee: MITSUBISHI MATERIALS CORPORATION
- Current Assignee Address: JP Tokyo
- Agency: Locke Lord LLP
- Agent James E. Armstrong, IV; Nicholas J. DiCeglie, Jr.
- Priority: JPP2009-082498 20090330
- International Application: PCT/JP2010/002308 WO 20100330
- International Announcement: WO2010/116682 WO 20101014
- Main IPC: B22F3/11
- IPC: B22F3/11 ; B22F7/00 ; C22C1/04 ; C22C1/08 ; C22C21/02 ; C22C21/12 ; C22C21/14 ; C22C21/16 ; H01G9/008 ; H01G11/68 ; H01G11/70 ; H01M4/66 ; H01M4/80 ; B22F1/00 ; B22F3/10

Abstract:
This method for producing porous sintered aluminum includes: mixing aluminum powder with a sintering aid powder containing titanium to obtain a raw aluminum mixed powder; mixing the raw aluminum mixed powder with a water-soluble resin binder, water, and a plasticizer containing at least one selected from polyhydric alcohols, ethers, and esters to obtain a viscous composition; drying the viscous composition in a state where air bubbles are mixed therein to obtain a formed object prior to sintering; and heating the formed object prior to sintering in a non-oxidizing atmosphere, wherein when a temperature at which the raw aluminum mixed powder starts to melt is expressed as Tm (° C.), a temperature T (° C.) of the heating fulfills Tm−10 (° C.)≦T≦685 (° C.).