- 专利标题: Lithium-ion secondary battery, electrode for the secondary battery, and electrolytic copper foil for electrode for the secondary battery
-
申请号: US13976503申请日: 2011-12-27
-
公开(公告)号: US09603245B2公开(公告)日: 2017-03-21
- 发明人: Akitoshi Suzuki , Kensaku Shinozaki , Toshio Tani , Hirokazu Sasaki , Isamu Futaba , Kouji Hataya , Shinya Ohtomo , Hirokazu Yoshikawa
- 申请人: Akitoshi Suzuki , Kensaku Shinozaki , Toshio Tani , Hirokazu Sasaki , Isamu Futaba , Kouji Hataya , Shinya Ohtomo , Hirokazu Yoshikawa
- 申请人地址: JP Tokyo
- 专利权人: FURUKAWA ELECTRIC CO., LTD.
- 当前专利权人: FURUKAWA ELECTRIC CO., LTD.
- 当前专利权人地址: JP Tokyo
- 代理机构: Kubotera & Associates, LLC
- 优先权: JP2010-290654 20101227
- 国际申请: PCT/JP2011/080314 WO 20111227
- 国际公布: WO2012/091060 WO 20120705
- 主分类号: H01M4/66
- IPC分类号: H01M4/66 ; H05K1/09 ; C22F1/08 ; C25D3/38 ; C25D5/48 ; C25D7/06 ; H01M4/133 ; H01M4/134 ; H01M4/1395 ; H01M10/0525 ; C23C22/24 ; C25D1/04 ; C25D5/10 ; C25D5/16 ; H01M4/04 ; H01M4/02
摘要:
To provide an electrolytic copper foil for a negative electrode for a lithium-ion secondary battery with which it is possible to produce a long-life lithium-ion secondary battery in which there is no decline in the capacity retention ratio even when the charge-discharge cycling is repeated, that has long life, and no deformation of a negative electrode current collector occurs. The electrolytic copper foil constituting the negative electrode current collector for the lithium-ion secondary battery has, after heat treatment at from 200 to 400° C., a 0.2% proof stress of 250 N/mm2 or more, and elongation of 2.5% or more; and the surface on which an active material layer of the electrolytic copper foil is provided has been rust-proofed, or roughened and rust-proofed. As a result of analysis of the depth profile (depth direction) obtained by performing secondary ion mass spectrometry (SIMS) in the thickness direction of the copper foil, the copper foil including: chlorine (Cl), carbon (C), and oxygen (O) each in a concentration of 1017 to 5×1020 atoms/cm3, and sulfur (S) and nitrogen (N) each in a concentration of 1015 to 1019 atoms/cm3.