摘要:
A cemented carbide material comprising tungsten carbide grains, the content of tungsten carbide in the cemented carbide material being at least 75 weight percent and at most 95 weight percent. The cemented carbide material comprises a binder phase comprising any of cobalt, iron, or nickel, and nanoparticles. Te nanoparticles include material according to the formula CoxWyCz, where x is a value in the range from 1 to 7, y is a value in the range from 1 to 10 and z is a value in the range from 0 to 4. The nanoparticles have a mean grain size of no more than 10 nm and at least 10 percent of the nanoparticles have a size of at most 5 nm. The volume percent of the tungsten carbide grains having a grain size of no more than 1 μm is less than 4 percent. A method for producing the cemented carbide material is also disclosed.
摘要:
A pick tool assembly comprising a working tip, a base and at least one wear protector element. The working tip is attached to the base and the base comprises an attachment member for coupling the base to a driving mechanism. The working tip comprises super-hard material, the base comprises a first material and the wear protector element comprises a second material having greater abrasive wear resistance than the first material. The base and wear protector element are cooperatively configured so that wear protector element is mechanically securable to the base.
摘要:
Cemented carbide material comprising tungsten carbide (WC) material in particulate form having a mean grain size D in terms of equivalent circle diameter of at least 0.5 microns and at most 10 microns, and a binder phase comprising cobalt (Co) of at least 5 weight per cent and at most 12 weight per cent, W being present in the binder at a content of at least 10 weight per cent of the binder material; the content of the WC material being at least 75 weight per cent and at most 95 weight per cent; and nanoparticles dispersed in the binder material, the nanoparticles comprising material according to the formula CoxWyCz, where X is a value in the range from 1 to 7, Y is a value in the range from 1 to 10 and Z is a value in the range from 0 to 4; the nanoparticles having a mean particle size at most 10 nm, at least 10 per cent of the nanoparticles having size of at most 5 nm; the cemented carbide material having a magnetic coercive force in the units kA/m of at least -2.1 X D + 14.
摘要:
A cemented carbide body is provided with improved resistance to mechanical fatigue. The cemented carbide body comprises tantalum in the binder matrix material. The tantalum content is between 1.5 weight per cent and 3.5 weight per cent of the binder content. The binder comprises tantalum-containing inclusions having a mean largest linear dimension of no more than 80 nm
摘要:
A method and granules for coating a body. Each granule comprises silicon (Si), carbon (C), chromium (Cr) and iron group metal selected from iron (Fe), cobalt (Co) and nickel (Ni). The relative quantities of the Si, C and Cr are such that a molten phase comprising the Si, C, Cr and the iron group metal will form at a melting temperature of less than 1,300 degrees Celsius when at least a threshold quantity of the iron group metal is accessible to the Si, C and Cr; but each granule comprising substantially less than the threshold quantity of the iron group metal. A second source of the iron group metal is provided. A combination of the granules and the second source is formed such that at least the threshold quantity of the iron group metal will be accessible to the Si, C and Cr. The granules and the second source are heated to at least the melting temperature to form the molten phase in contact with the body. The heat is then removed to allow the molten phase to solidify and to provide the coated body.
摘要:
A pick tool comprising a super-hard strike tip, a base and a unitary cemented carbide support body comprising a head portion including an overhang portion, and an insertion shaft extending from the head portion, a surface of the overhang portion extending laterally from the insertion shaft; the strike tip is attached to the head portion of the support body and the base is provided with a bore into which the insertion shaft is shrink fitted; the base has an external surface adjacent the bore and overhang portion of the head portion is configured to extend over at least an area of the external surface operative to shield the area from wear when in use.
摘要:
An insert (110) for a degradation assembly comprising a holder, the insert (110) comprising a tip (112), a coupler mechanism (114) for moveably coupling the insert with the holder, and an alignment mechanism operable to urge the tip (112) towards an aligned orientation within the holder; the aligned orientation being with respect to a forward direction (M) in which the insert (110) is to be driven in use.
摘要:
A body comprising a steel substrate and a hard face structure fused to the steel substrate, in which the hard face structure comprises at least 1 weight percent Si, at least 5 weight percent Cr and at least 40 weight percent W and substantially the balance of the hard face structure consisting essentially of an iron group metal M and C, M being selected from Fe, Co and Ni or an alloy thereof; the hard face structure including a plurality of elongate or platelike micro-structures having a mean length of at least 1 micron, a plurality of nano-particles having a mean size of less than 200 nanometres, and a binder material; the micro-structures comprising more than 1 weight percent Cr and a phase having the formula M x W y C z , where x is in the range from 1 to 7, y is in the range from 1 to 10 and z is in the range from 1 to 4; the nano- particles comprising more than 20 weight percent W, the metal M, and C; and the binder material comprising more than 3 weight percent W, more than 2 weight percent Cr, more than 0.5 weight percent Si, the metal M and C.