METHOD OF MOLDING RIGID POLYURETHANE FOAMS WITH ENHANCED THERMAL CONDUCTIVITY
    13.
    发明授权
    METHOD OF MOLDING RIGID POLYURETHANE FOAMS WITH ENHANCED THERMAL CONDUCTIVITY 有权
    具有增强的导热性的刚性聚氨酯泡沫体的成型方法

    公开(公告)号:EP1951777B1

    公开(公告)日:2017-05-17

    申请号:EP06827462.0

    申请日:2006-11-03

    摘要: The present invention is to a process of producing a molded rigid polyurethane foam for application in appliance, having a reduced thermal conductivity at densities between 33 and 38 kg/m 3 . The molded rigid polyurethane foam have a ratio of applied foam density (kg/m 3 ) to lambda (mW/mK), measured at 10°C, 24 hours after foam production from 1.65 and to 2.15 and are obtained by the process of injecting into a closed mold cavity under reduced pressure a reaction mixture at a packing factor of 1.1 to 1.9 and the reaction mixture comprises: A) an organic polyisocyanate; B) a physical blowing agent; C) a polyol composition containing at least one polyol with a functionality of 3 or greater and a hydroxyl number between 200 and 800 and a water content of 0 to 2.5 weight percent of the total polyol composition; D) catalyst; and E) auxiliary substances and/or additives.

    摘要翻译: 本发明涉及一种应用于器具的模制硬质聚氨酯泡沫体,其密度在33和38kg / m 3之间时具有降低的热导率,以及用于生产这种泡沫体的方法。 所述模制的硬质聚氨酯泡沫体在10℃,泡沫体生产后24小时测量的泡沫体密度(kg / m 3)与λ(mW / mK)的比率为1.65至2.15,并且通过注射 在减压下将填料系数为1.1-1.9的反应混合物注入封闭的模腔中,反应混合物包含:A)有机多异氰酸酯; B)物理发泡剂,C)多元醇组合物,其包含至少一种官能度为3或更大且羟值为200至800且多元醇组合物的总含水量为0至2.5重量%的多元醇; D)催化剂和E)辅助物质和/或添加剂。