Abstract:
A catalyst composition comprises a self-bound zeolite and a Group 12 transition metal selected from the group consisting of Zn, Cd, or a combination thereof, the zeolite having a silicon to aluminum ratio of at least about 10, the catalyst composition having a micropore surface area of at least about 340 m2/g, a molar ratio of Group 12 transition metal to aluminum of about 0.1 to about 1.3, and at least one of: (a) a mesoporosity of greater than about 20 m2/g; (b) a diffusivity for 2,2-dimethylbutane of greater than about 1×10−2 sec−1 when measured at a temperature of about 120° C. and a 2,2-dimethylbutane pressure of about 60 torr (about 8 kPa).
Abstract:
A supported catalyst comprises a zeolite having a silica to alumina molar ratio of 500 or less, a first metal oxide binder having a crystallite size greater than 200 Å and a second metal oxide binder having a crystallite size less than 100 Å, wherein the second metal oxide binder is present in an amount less than 15 wt % of the total weight of the catalyst.
Abstract:
Apparatuses and processes for converting an oxygenate feedstock, such as methanol and dimethyl ether, in a fluidized bed containing a catalyst to hydrocarbons, such as gasoline boiling components, olefins and aromatics are provided herein.
Abstract:
A catalyst composition comprises a self-bound zeolite and a Group 12 transition metal selected from the group consisting of Zn, Cd, or a combination thereof, the zeolite having a silicon to aluminum ratio of at least about 10, the catalyst composition having a micropore surface area of at least about 340 m2/g, a molar ratio of Group 12 transition metal to aluminum of about 0.1 to about 1.3, and at least one of: (a) a mesoporosity of greater than about 20 m2/g; (b) a diffusivity for 2,2-dimethylbutane of greater than about 1×10−2 sec−1 when measured at a temperature of about 120° C. and a 2,2-dimethylbutane pressure of about 60 torr (about 8 kPa).
Abstract:
A catalyst composition comprises a self-bound zeolite and a Group 12 transition metal selected from the group consisting of Zn, Cd, or a combination thereof, the zeolite having a silicon to aluminum ratio of at least about 10, the catalyst composition having a micropore surface area of at least about 340 m2/g, a molar ratio of Group 12 transition metal to aluminum of about 0.1 to about 1.3, and at least one of: (a) a mesoporosity of greater than about 20 m2/g; (b) a diffusivity for 2,2-dimethylbutane of greater than about 1×10−2 sec−1 when measured at a temperature of about 120° C. and a 2,2-dimethylbutane pressure of about 60 torr (about 8 kPa).
Abstract:
A catalyst composition comprises a self-bound zeolite and a Group 12 transition metal selected from the group consisting of Zn, Cd, or a combination thereof, the zeolite having a silicon to aluminum ratio of at least about 10, the catalyst composition having a micropore surface area of at least about 340 m2/g, a molar ratio of Group 12 transition metal to aluminum of about 0.1 to about 1.3, and at least one of: (a) a mesoporosity of greater than about 20 m2/g; (b) a diffusivity for 2,2-dimethylbutane of greater than about 1×10−2 sec−1 when measured at a temperature of about 120° C. and a 2,2-dimethylbutane pressure of about 60 torr (about 8 kPa).