OXIDE DIELECTRIC AND METHOD FOR MANUFACTURING SAME, AND SOLID STATE ELECTRONIC DEVICE AND METHOD FOR MANUFACTURING SAME
    11.
    发明公开
    OXIDE DIELECTRIC AND METHOD FOR MANUFACTURING SAME, AND SOLID STATE ELECTRONIC DEVICE AND METHOD FOR MANUFACTURING SAME 审中-公开
    氧化物电介质及其制造方法体和电子固态装置和方法及其生产

    公开(公告)号:EP3173381A1

    公开(公告)日:2017-05-31

    申请号:EP15823922.8

    申请日:2015-07-10

    IPC分类号: C01G33/00 C04B35/00 H01G4/12

    摘要: There are provided an oxide dielectric having excellent properties and a solid state electronic device (e.g., a capacitor, a semiconductor device, or a small electromechanical system) having such an oxide dielectric.
    An oxide layer 30 includes an oxide dielectric (possibly including inevitable impurities) including bismuth (Bi) and niobium (Nb) and having a first crystal phase of a pyrochlore-type crystal structure and a second crystal phase of a β-BiNbO 4 -type crystal structure. The oxide layer 30 has a controlled content of the first crystal phase and a controlled content of the second crystal phase, in which the first crystal phase has a dielectric constant that decreases with increasing temperature of the oxide layer 30 in a temperature range of 25°C or more and 120°C or less, and the second crystal phase has a dielectric constant that increases with increasing temperature of the oxide layer 30 in the temperature range.

    摘要翻译: 本发明提供在具有优异的性能和固态电子装置(E. G.,电容器,半导体装置,或较小的机电系统),其具有检测上氧化物电介质的介电氧化物。 氧化物层30包括氧化物介电(可能包括不可避免的杂质)包含铋(Bi)和铌(Nb)和具有烧绿石型晶体结构的第一晶体相和²-宾波4型的第二晶相 晶体结构。 该氧化物层30具有与第一晶相的控制的内容和第二晶相的控制的内容,其中,所述第一结晶相的介电常数所做降低了与在一个温度范围内的25°增加氧化物层30的温度 ℃或更高和120℃或以下,并且第二晶相的介电常数做了与在所述温度范围增加氧化物层30的温度增加。

    ELECTRICITY-GENERATING DEVICE
    13.
    发明公开

    公开(公告)号:EP3171488A4

    公开(公告)日:2018-03-07

    申请号:EP15822158

    申请日:2015-07-09

    申请人: ADAMANT CO LTD

    发明人: AOYAGI TOMOHIDE

    摘要: Provided is a power generating device which, while having a basic structure of using a rack and a pinion, increases power generating efficiency and has fewer components, has improved durability due to a simplified structure, and can easily be made in smaller sizes. Configuring a guide mechanism using outer walls of a case of a power generating unit as guides and combining the same with rails provided on inner walls of a case of the power generating device distributes unnecessary stress on the power generating unit over the inner walls of the case to obtain effects of achieving an overall small size, reduction in the number of components, and improved durability.

    CURRENT MEASURING DEVICE
    15.
    发明公开
    CURRENT MEASURING DEVICE 审中-公开
    电流测量装置

    公开(公告)号:EP2966459A1

    公开(公告)日:2016-01-13

    申请号:EP14760774.1

    申请日:2014-02-27

    申请人: Adamant Co., Ltd.

    IPC分类号: G01R15/24

    摘要: Provided is a current measuring device such that it is possible to reliably keep the fluctuation range for the ratio error in output to within a range of ±0.5% and such that assembly thereof can be simplified. The current measuring device is configured to include at least a light entrance and exit, an optical fiber for a sensor, a Faraday rotator, a first 1/4 wavelength plate, a second 1/4 wavelength plate, a polarization separator, a light source, and a signal processing circuit comprising a photoelectric conversion element. The optical fiber for a sensor has birefringence and comprises one end into which two circularly polarized light beams having different directions of rotation enter and another end that reflects the circularly polarized light beams that have entered. In addition, the phase difference of two linearly polarized light beams in the round-trip light path between the two 1/4 wavelength plates is compensated, and the Faraday rotational angle when the Faraday rotator is magnetically saturated is set to 22.5°+α° so that the fluctuation range for the ratio error in the measured value of the current to be measured is set to be in the range of ±0.5%. In addition, the crystal axes on the optical faces of the two 1/4 wavelength plates are set to be perpendicular or are set to be in the same direction.

    摘要翻译: 提供一种电流测量装置,使得可以可靠地将输出中的比率误差的波动范围保持在±0.5%的范围内,并且可以简化组装。 电流测量装置被配置为至少包括光入口和出口,用于传感器的光纤,法拉第旋转器,第一1/4波长板,第二1/4波长板,偏振分离器,光源 以及包括光电转换元件的信号处理电路。 用于传感器的光纤具有双折射并且包括具有不同旋转方向的两个圆偏振光束进入的一端和反射已经进入的圆偏振光束的另一端。 另外,两个1/4波长板之间的往返光路中的两个线性偏振光束的相位差被补偿,并且当法拉第转子磁饱和时的法拉第转角被设置为22.5°+α° 使得待测电流的测量值中的比率误差的波动范围被设定在±0.5%的范围内。 此外,两个1/4波长板的光学面上的晶轴被设置为垂直或设置在相同的方向上。

    SLEEVE FOR OPTICAL COMMUNICATION, AND METHOD FOR MANUFACTURE FOR SAME SLEEVE FOR OPTICAL COMMUNICATION
    16.
    发明公开
    SLEEVE FOR OPTICAL COMMUNICATION, AND METHOD FOR MANUFACTURE FOR SAME SLEEVE FOR OPTICAL COMMUNICATION 审中-公开
    JACK用于生产灌木丛中光通信光通信方法

    公开(公告)号:EP2860559A1

    公开(公告)日:2015-04-15

    申请号:EP13800438.7

    申请日:2013-06-05

    申请人: Adamant Co., Ltd.

    摘要: Provided are a sleeve for optical communication and method for manufacture for the sleeve for optical communication, for which withdrawal force for ferrules, which are generally used in the technical field of optical communication, or connection loss between ferrules is a predetermined value, and for which manufacturing steps are reduced so as to allow reduction of manufacturing cost. The present invention is made by press-molding ceramic feedstock, which after cold isostatic pressing and sintering are performed thereto, and is made so that an inner circumferential surface (4a), of a through-hole (2a) for inserting a ferrule formed on the length-direction of the axis, has a sintered state.

    摘要翻译: 提供了用于制造用于套筒用于光通信的光通信和方法的套筒,用于套圈,这是在光通信,或套圈之间的连接损耗的技术领域中使用的基因的反弹哪个拔出力是预定值,和对于哪 制造步骤减少,从而允许降低制造成本。 本发明是通过加压成形陶瓷原料,其中冷等静压压制和烧结后进行对其做出,并且被制造成用于插入形成于套箍做了通孔(2a)的内圆周表面(4a)的 轴的长度方向上,具有烧结状态。