TERMINAL-MODIFIED POLYAMIDE RESIN, METHOD FOR PRODUCING SAME, AND METHOD FOR PRODUCING MOLDED ARTICLES
    19.
    发明公开
    TERMINAL-MODIFIED POLYAMIDE RESIN, METHOD FOR PRODUCING SAME, AND METHOD FOR PRODUCING MOLDED ARTICLES 审中-公开
    末端改性的聚酰胺树脂,用于生产及其制造方法形状的物体

    公开(公告)号:EP3150654A1

    公开(公告)日:2017-04-05

    申请号:EP15800376.4

    申请日:2015-05-28

    IPC分类号: C08G69/40 C08L77/00

    摘要: The present invention addresses the problem of providing a high molecular weight, terminal modified polyamide resin having a low melt viscosity and excellent molding processability.
    The problem is solved by a terminal modified polyamide resin having a relative viscosity (ηr), as measured at 25°C in a 98% sulfuric acid solution at a resin concentration of 0.01 g/ml, of 2.1 to 10, the resin comprising 0.05 to 4.5% by mass of a terminal structure represented by general formula (I):

            -X-(R 1 -O) n -R 2      (I)

    wherein n ranges from 2 to 100; R 1 represents a hydrocarbon group of 2 to 10 carbon atoms; R 2 represents a hydrocarbon group of 1 to 30 carbon atoms; -X- represents - NH- or -N(CH 3 )-; and n R 1 s in the general formula (I) may be the same or different.

    摘要翻译: 本发明解决了这个问题,提供的高分子量,具有低熔融粘度和优异的模塑加工性末端改性聚酰胺树脂。 麻烦的是由具有相对粘度(* R)末端改性聚酰胺树脂解决了,在98%的硫酸溶液在0.01克的树脂浓度在25℃下所测量/ ml时,为2.1〜10中,树脂包括 0点05分至4.5%的由通式(I)所示的末端结构的质量:€€ƒƒƒ€€€ƒƒƒ€€€ƒƒ-X-(R 1 -O)N -R 2€ƒ€ ƒƒ€€€ƒƒ(I)worin n的范围为2至100; R 1表示的含2-10个碳原子的烃基; R 2 darstellt的烃基的1〜30个碳原子; -X- darstellt - NH-或-N(CH 3) - ; 和n个R 1的通式(I)中可以是相同的或不同的。

    COMPOSITION DE COPOLYAMIDE A MAIN SOUPLE
    20.
    发明公开
    COMPOSITION DE COPOLYAMIDE A MAIN SOUPLE 审中-公开
    共聚乳酸锌麻醉剂

    公开(公告)号:EP3134476A1

    公开(公告)日:2017-03-01

    申请号:EP15714572.3

    申请日:2015-03-05

    申请人: Arkema France

    摘要: Composition comprising, by weight, the total being equal to 100%: from 98% to 100% of at least one copolyamide comprising amide units and polyether units, having a melting point (Mp) from approximately 90 to approximately 150°C, in particular from approximately 100°C to approximately 125°C, and having a flexural modulus of less than 100 MPa, as determined according to standard ISO 178 (2010); - from 0 to 2% of at least one additive chosen from stabilizers and dyes, or a mixture thereof, for the manufacture of a heat-sensitive adhesive, in particular a web, a film, granules, a filament, a grid, a powder or a suspension.

    摘要翻译: 组合物包含总重量等于100%:98%至100%的至少一种包含酰胺单元和聚醚单元的共聚酰胺,其熔点(Mp)为约90至约150℃,特别是 从约100℃至约125℃,并且具有小于100MPa的挠曲模量,如根据标准ISO 178(2010)所测定的; - 选自稳定剂和染料的至少一种添加剂的0至2%,或其混合物,用于制造热敏粘合剂,特别是纤维网,膜,颗粒,丝,网格,粉末 或暂停。