LOW-LEAD BRASS ALLOY FOR PLUMBING MEMBER
    31.
    发明公开
    LOW-LEAD BRASS ALLOY FOR PLUMBING MEMBER 审中-公开
    BLEIARME MESSINGLEGIERUNGFÜRSANITÄREELEMENT

    公开(公告)号:EP3128020A4

    公开(公告)日:2017-04-12

    申请号:EP15772552

    申请日:2015-03-06

    申请人: KURIMOTO LTD

    IPC分类号: C22C9/04

    CPC分类号: C22C9/04

    摘要: An object of the present invention is to provide a brass alloy, in which the content of Bi is reduced to secure a good recyclability while maintaining the dezincification corrosion resistance required for a member for water works, and which is capable of exhibiting an erosion-corrosion resistance and excellent mechanical properties to be used as a member for water works. This brass alloy contains: 24% by mass or more and 34% by mass or less of Zn; 0.5% by mass or more and 1.7% by mass or less of Sn; 0.4% by mass or more and 1.8% by mass or less of Al; 0.005% by mass or more and 0.2% by mass or less of P; and 0.01% by mass or more and 0.25% by mass or less of Pb; with the balance being copper and an unavoidable impurity(ies). Note, however, that in cases where the above mentioned copper alloy has a content of Sn of less than 1.0% by mass, the contents of Al and Sn in % by mass satisfy the Inequality: Al + 2 × Sn ‰¥ 2.8.

    摘要翻译: 本发明的一个目的是提供一种黄铜合金,其中降低Bi的含量以确保良好的可再循环性,同时保持用于水厂的构件所需的抗脱锌腐蚀性,并且能够表现出腐蚀腐蚀 耐水性和优良的机械性能,可用作水厂的一员。 该黄铜合金含有24质量%以上且34质量%以下的Zn, Sn:0.5质量%以上且1.7质量%以下; Al:0.4质量%以上且1.8质量%以下; P:0.005质量%以上且0.2质量%以下; 和0.01质量%以上且0.25质量%以下的Pb; 其余为铜和不可避免的杂质。 但是,在上述铜合金的Sn含量小于1.0质量%的情况下,Al和Sn的含量的质量百分比满足不等式:Al + 2×Sn≥0.8。

    KNEADING AND STIRRING DEVICE
    33.
    发明公开
    KNEADING AND STIRRING DEVICE 审中-公开
    KNET- UNDRÜHRRORRICHTUNG

    公开(公告)号:EP2732870A1

    公开(公告)日:2014-05-21

    申请号:EP12811585.4

    申请日:2012-06-04

    申请人: Kurimoto, Ltd.

    IPC分类号: B01F7/02 B01F15/00

    摘要: A kneader/stirrer is provided which has a high self-cleaning ability and can be operated for a long period of time. The kneader/stirrer includes two rotary shafts (4) extending parallel to each other in the processing chamber (2), first regular triangular impellers (3) mounted to one of the rotary shafts (4) so as to be arranged in the axial direction of the rotary shaft (4), and second regular triangular impellers (3) mounted to the other rotary shaft (4) at the same axial positions as the respective first impellers (3). The impellers (3) are fixed to the respective rotary shafts (4) at points offset from the centers of the respective impellers (3) in a predetermined direction by a predetermined distance such that when the two rotary shafts (4) rotate in the same direction at the same speed, each pair of first and second impellers (3) are eccentrically pivoted, with one apex of one of the pair of impellers kept in contact with or in close proximity to the contour of the other impeller, thereby scraping off polycondensation resin (material to be processed) adhered to the other impeller, while scraping off resin adhered to the inner wall of the processing chamber (2) with one of the apexes nearest to the inner wall. Thus, this device has a higher self-cleaning ability than conventional devices using disk-shaped impellers, and thus can be stably operated for a long period of time.

    摘要翻译: 提供了具有高自清洁能力并可长时间操作的捏合机/搅拌器。 捏合机/搅拌机包括在处理室(2)中彼此平行延伸的两个旋转轴(4),安装在一个旋转轴(4)上的第一规则三角形叶轮(3),以沿轴向方向 以及在与第一叶轮(3)相同的轴向位置处安装到另一旋转轴(4)的第二规则三角形叶轮(3)。 叶轮(3)在预定方向上偏离各叶轮(3)的中心的点处固定到相应的旋转轴(4)上预定距离,使得当两个旋转轴(4)在同一旋转轴 方向以相同的速度,每对第一和第二叶轮(3)偏心地枢转,一对叶轮中的一个叶轮的一个顶点与另一个叶轮的轮廓保持接触或非常接近,从而刮除缩聚 树脂(待处理材料)粘附到另一个叶轮上,同时用最靠近内壁的顶点之一刮去附着在处理室(2)的内壁上的树脂。 因此,该装置具有比使用盘形叶轮的常规装置更高的自清洁能力,因此可以长时间稳定地操作。

    METAL THIN PLATE JOINING METHOD AND METAL THIN PLATE JOINT STRUCTURE

    公开(公告)号:EP3406390A1

    公开(公告)日:2018-11-28

    申请号:EP18740496.7

    申请日:2018-02-05

    申请人: Kurimoto, Ltd.

    IPC分类号: B23K20/12

    摘要: A first metal sheet (1) is placed on a backing metal plate (6), and an end portion of a second metal sheet (2) is placed on top of an end portion of the first metal sheet (1) such that the ends of the end portions are spaced apart from each other by a predetermined distance in side view. The end portions of the first and second metal sheets (1) and (2) are joined together by downwardly pressing a rotating rotary tool (4) onto the end portion of the second metal sheet (2) placed on top of the end portion of the first metal sheet (1) and by utilizing frictional heat and pressurizing force generated between the rotating tool and the first and second metal sheets (1) and (2).

    LOW-LEAD BRASS ALLOY FOR PLUMBING MEMBER
    39.
    发明公开
    LOW-LEAD BRASS ALLOY FOR PLUMBING MEMBER 审中-公开
    用于管件的低铅黄铜合金

    公开(公告)号:EP3128020A1

    公开(公告)日:2017-02-08

    申请号:EP15772552.4

    申请日:2015-03-06

    申请人: Kurimoto, Ltd.

    IPC分类号: C22C9/04

    CPC分类号: C22C9/04

    摘要: An object of the present invention is to provide a brass alloy, in which the content of Bi is reduced to secure a good recyclability while maintaining the dezincification corrosion resistance required for a member for water works, and which is capable of exhibiting an erosion-corrosion resistance and excellent mechanical properties to be used as a member for water works. This brass alloy contains: 24% by mass or more and 34% by mass or less of Zn; 0.5% by mass or more and 1.7% by mass or less of Sn; 0.4% by mass or more and 1.8% by mass or less of Al; 0.005% by mass or more and 0.2% by mass or less of P; and 0.01% by mass or more and 0.25% by mass or less of Pb; with the balance being copper and an unavoidable impurity(ies). Note, however, that in cases where the above mentioned copper alloy has a content of Sn of less than 1.0% by mass, the contents of Al and Sn in % by mass satisfy the Inequality: Al + 2 × Sn ≥ 2.8.

    摘要翻译: 本发明的一个目的是提供一种黄铜合金,其中降低Bi的含量以确保良好的可再循环性,同时保持用于水厂的构件所需的抗脱锌腐蚀性,并且能够表现出腐蚀腐蚀 耐水性和优良的机械性能,可用作水厂的一员。 该黄铜合金含有24质量%以上且34质量%以下的Zn, Sn:0.5质量%以上且1.7质量%以下; Al:0.4质量%以上且1.8质量%以下; P:0.005质量%以上且0.2质量%以下; 和0.01质量%以上且0.25质量%以下的Pb; 其余为铜和不可避免的杂质。 但是,在上述铜合金的Sn含量小于1.0质量%的情况下,Al和Sn的含量以质量%计满足不等式:Al + 2×Sn≥2.8。