摘要:
A carpet includes (a) a primary backing which has a face and a back surface, (b) a plurality of fibers attached to the primary backing and extending from the face of the primary backing and exposed at the back surface of the primary backing, (c) an adhesive backing, (d) an optional secondary backing adjacent to the adhesive backing, and (e) at least one olefin block copolymer, especially ethylene based block copolymers. An olefin block copolymer is extrusion coated onto the back surface of a primary backing to provide an adhesive backing. Additional steps and procedures can include washing or scouring the primary backing and fibers prior to the extrusion step, and utilizing implosion agents. The preferred olefin block copolymer is an ethylene based block interpolymer. The constructions and methods are suited for making tufted, broad-loom carpet having improved abrasion resistance.
摘要:
The present invention relates to a composition comprising an ethylene/alpha-olefin interpolymer, and wherein the ethylene/alpha-olefin interpolymer comprises the following properties: a) an HCC value less than, or equal to, 4.4%; and b) a highest peak melting temperature less than, or equal to, 72.0°C.
摘要:
Flooding compounds for telecommunications cables. Such flooding compounds contain a polyolefin elastomer and a hydrocarbon oil. The polyolefin elastomer has a crystallinity ranging from 10 less than 50 weight percent and a dynamic viscosity of 50,000 centipoise or less at 177° C. The hydrocarbon oil has a kinematic viscosity of 200 centistokes or less at 40° C.
摘要:
Flooding compounds for telecommunications cables. Such flooding compounds contain a polymeric filler and a branched olefinic fluid. The branched olefinic fluid has an average of at least 1.5 methine carbons per oligomer molecule and at least 40 methine carbons per one thousand total carbons. Additionally, the average number of carbons per molecule in the branched olefinic fluid is from 25 to 200.
摘要:
A hot melt adhesive composition includes (A) 10-95 wt % of a random or homogeneous propylene-based interpolymer having: (i) a comonomer content of at least one of C2 and C4-10 a-olefin of 7 wt % to 49 wt % based on the total weight of the propylene-based interpolymer, (ii) an MWD of 4 or less, (iii) a density of 0.90 g/cc or less, and (iv) a Brookfield viscosity of less than 50,000 centipoise, (B) 1-60 wt % of a crystalline block composite comprising: (1) a crystalline ethylene based polymer; (2) a crystalline alpha-olefin based polymer derived from at least one of a C3-10 a-olefin; and (3) a block copolymer comprising 10-90 wt % of a crystalline ethylene block comprising greater than 90 mol % units derived from ethylene and comprising 10-90 wt % of a crystalline alpha-olefin block comprising greater than 90 mol % units derived from at least one of a C3-10 a-olefin, (C) Optionally, from greater than zero to 70 wt % tackifier, and (D) Optionally, from greater than zero to 40 wt % of at least one selected from the group of a wax and an oil.