Abstract:
An amorphous alloy having the general formula of: (ZrxAlyCuzNi1-x-y-z)100-a-bScaYb, wherein x, y, and z are atomic percents, and a and b are atom molar ratios, in which: about 0.45≦̸x≦̸about 0.60; about 0.08≦̸y≦̸about 0.12; about 0.25≦̸z≦̸about 0.35; 0
Abstract:
A method for integrally molding a metal and a resin and a metal-resin composite structure obtainable by the same are provided. The method comprises forming a nanopore in a surface of a metal sheet; melting a thermoplastic resin on the surface of the metal sheet formed with the nanopore; and injection molding the thermoplastic resin onto the surface of the metal sheet. The thermoplastic resin is a mixture of a main resin and a polyolefin resin, the main resin is a mixture of polyphenylene oxide and a polyamide, and the polyolefin resin has a melting point of about 65° C. to about 105° C.
Abstract:
A metal-ceramic composite includes a ceramic substrate and a metallic composite. A groove is formed in a surface of the ceramic substrate and the metallic composite is filled in the groove. The metallic composite includes a Zr based alloy-A composite. A includes at least one selected from a group consisting of W, Mo, Ni, Cr, stainless steel, WC, TiC, SiC, ZrC and ZrO 2 . Based on the total volume of the Zr based alloy-A composite, the content of A is about30%to about70%by volume.A method for preparing the metal-ceramic composite is also provided.
Abstract:
A metal-resin composite and method for producing the same are provided. The method comprises steps of: A) forming nanopores in at least a part of the surface of a shaped metal; and B) injection molding a thermoplastic resin directly on the surface of the shaped metal, wherein the 5 thermoplastic resin includes a main resin and a polyolefin resin, the main resin includes a mixture of polyphenylene ether and polyphenylene sulfide, and the polyolefin resin has a melting point of about 65§ to about 105§.
Abstract:
A method for integrally molding a metal and a resin and a metal-resin composite structure obtainable by the same are provided. The method comprises forming a nanopore in a surface of a metal sheet; melting a thermoplastic resin on the surface of the metal sheet formed with the nanopore; and injection molding the thermoplastic resin onto the surface of the metal sheet. The thermoplastic resin is a mixture of a main resin and a polyolefin resin, the main resin is a mixture of polyphenylene oxide and a polyamide, and the polyolefin resin has a melting point of about 65° C. to about 105° C.
Abstract:
A sealing assembly, a method of preparing the sealing assembly and a battery are provided. The sealing assembly comprises a metal ring (1) having a mounting hole therein; a ceramic ring (2) having a connecting hole therein and disposed in the mounting hole; and a core column (3) disposed in the connecting hole, wherein at least one of an inner circumferential wall surface of the metal ring, an outer circumferential wall surface of the ceramic ring, an inner circumferential wall surface of the ceramic ring and an outer circumferential wall surface of the core column is configured as an inclined surface, and an inclination angle of the inclined surface relative to a vertical plane is about 1 degree to about 45 degrees.
Abstract:
A zirconium (Zr)-based amorphous alloy and a preparing method thereof are provided. The Zr-based amorphous alloy is represented by the general formula of (Zr a M b N c ) 100-x Q x , in which M is at least one transition metal except Zr; N is Be or Al; Q is selected from the group consisting of CaO, MgO, Y 2 O 3 , Nd 2 O 3 and combinations thereof; a, b and c are atomic percents of corresponding elements; and 45≤a≤75, 20≤b≤40, 1≤c≤25, a+b+c=100, and 1≤x≤15. A method for recycling a Zr-based amorphous alloy is also provided.