摘要:
Fine particles of a phosphor are weighed, mixed, and filled. Provided after this step are at least one step of firing the particles in a reducing atmosphere, and a step of pulverizing, dispersing, rinsing, drying and then treating the particles in an oxygen plasma atmosphere after the last step of treatment in the reducing atmosphere. This method recovers oxygen vacancy in the host crystal of the phosphor.
摘要:
The present invention aims at realizing a PDP and a mercury-free fluorescent lamp feasible to maintain excellent luminescent characteristics over long periods by suppressing time-lapse changes in luminescent characteristics of a phosphor that is excited by vacuum ultraviolet light to thereby emit light. To accomplish this object, the oxide phosphor of the invention comprises individual particles, each of which has a region at and near the surface thereof modified, and the elemental composition of the surface region is in a more oxidized state than that of the internal region of the particles. Alternatively, the surface region has more halogen or chalcogen in the elemental composition. In the phosphor treatment method of the invention, the surface region of individual phosphor particles is selectively modified by (i) forming a highly reactive gas atmosphere by exciting gas which contains reactive gas, and (ii) exposing the phosphor to the gas atmosphere.
摘要:
Fine particles of a phosphor are weighed, mixed, and filled. Provided after this step are at least one step of firing the particles in a reducing atmosphere, and a step of pulverizing, dispersing, rinsing, drying and then performing oxygen ion implantation treatment for implanting oxygen ions and annealing the particles, after the step of treatment in the reducing atmosphere. This method recovers oxygen vacancy in the host crystal of the phosphor.
摘要:
In a phosphor whose host crystal is constituted of an oxide, a method of preparing the phosphor where the oxygen deficiencies in the phosphor are not many, and a plasma display device using the same are provided. After processes of weighing, mixing and filling powders of the phosphor, a process for firing in a reducing atmosphere and a process for firing in an oxidizing atmosphere after the last reducing atmosphere process are provided. In addition, a firing temperature in the oxidizing atmosphere process is not less than 600 °C and not more than 1000 °C.
摘要:
A method and composition for manufacturing a luminescent screen (22) assembly for a color cathode ray tube (CRT) (10) is disclosed. The luminescent screen assembly is formed on an interior surface of a faceplate panel of the CRT. The luminescent screen assembly has a patterned light-absorbing matrix (23) thereon. The matrix defines a first set of fields (40), a second set of fields (42), and a third set of fields (44). An aqueous pigment suspension is applied to the first set of fields. The aqueous pigment suspension comprises a pigment, one or more surface-active agents and at least one non-pigmented oxide particle. The at least one non-pigmented oxide particle has a size that is less than that of the pigment.
摘要:
Fine particles of a phosphor are weighed, mixed, and filled. Provided after this step are at least one step of firing the particles in a reducing atmosphere, and a step of pulverizing, dispersing, rinsing, drying and then treating the particles in an ozone atmosphere after the last step of treatment in the reducing atmosphere. This method recovers oxygen vacancy in the host crystal of the phosphor.
摘要:
An improvement of a phosphor layer in mainly the luminance and chromaticity of plasma displays by using phosphor particles which are platy or have an appropriate particle diameter distribution to thereby increase the percentage of loading with the phosphor particles. In an aluminate phosphor containing barium as a base material and europium as an activator, the amount of europium serving as a luminescence center is controlled by using base materials in an appropriate proportion, and heat resistance is improved by appropriately regulating the amount of europium replacement, and durability is improved by appropriately regulating the amount of strontium replacement.