公开(公告)号:EP0102725A2
公开(公告)日:1984-03-14
申请号:EP83304201.3
申请日:1983-07-20
CPC分类号: C22B3/06 , C22B15/0067 , C22B15/0069 , C22B19/22 , Y02P10/234 , Y02P10/236
摘要: A process for the hydrometallurgical recovery of metal value, particularly copper, from copper-containing sulphide materials in which the material is conventionally ground and reacted with a solution containing less than 3 moles per litre of chloride ion, and optionally as little as 15 g/litre, together with sulphate ions with continuous oxygen injection and vigerous agitation. The reacting may be carried out at a pH in the range of 0.5 - 4, at moderate pressure as low as atmospheric pressure and at a moderate temperature below the boiling point of the solution such as 85°C.
-
公开(公告)号:EP0102725A3
公开(公告)日:1985-01-30
申请号:EP83304201
申请日:1983-07-20
CPC分类号: C22B3/06 , C22B15/0067 , C22B15/0069 , C22B19/22 , Y02P10/234 , Y02P10/236
摘要: A process for the hydrometallurgical recovery of metal value, particularly copper, from copper-containing sulphide materials in which the material is conventionally ground and reacted with a solution containing less than 3 moles per litre of chloride ion, and optionally as little as 15 g/litre, together with sulphate ions with continuous oxygen injection and vigerous agitation. The reacting may be carried out at a pH in the range of 0.5 - 4, at moderate pressure as low as atmospheric pressure and at a moderate temperature below the boiling point of the solution such as 85°C.
-