摘要:
A method and system for producing metallic iron nuggets may include providing multiple layers of agglomerates, such as briquettes, balls and extrusions, of a reducible mixture of reducing material (such as carbonaceous material) and of a reducible iron bearing material (such as iron oxide) on a hearth material layer (such as carbonaceous material) and providing a coarse overlayer of carbonaceous material over at least some of the agglomerates. Heating the agglomerates of reducible mixture to 1425 °C or 1400 °C or 1375 °C results in formation of an intermediate product of one or more metallic iron nuggets, which may have a sulfur content of less than 0.03%, and slag, which may have less than 5% mass MgO, which may have a ratio of percent by weight sulfur in the slag over percent by weight sulfur in the metallic nuggets of at least about 12 or at least about 15.
摘要:
Method and system for producing metallic nuggets includes providing reducible mixture (e.g., reducible micro-agglomerates; reducing material and reducible iron bearing material; reducible mixture including additives such as a fluxing agent; compacts, etc.) on at least a portion of a hearth material layer. In one embodiment, a plurality of channel openings extend at least partially through a layer of the reducible mixture to define a plurality of nugget forming reducible material regions. Such channel openings may be at least partially filled with nugget separation fill material (e.g., carbonaceous material). Thermally treating the layer of reducible mixture results in formation of one or more metallic iron nuggets. In other embodiments, various compositions of the reducible mixture and the formation of the reducible mixture provide one or more beneficial characteristics.
摘要:
Method and system for producing metallic nuggets includes providing reducible mixture of reducing material (such as carbonaceous material) and reducible iron bearing material (such as iron oxide) arranged in a plurality of discrete portions, such as mounds or briquettes, on at least a portion of a hearth material layer (such as carbonaceous material). An overlayer of turbulent gas flow disrupting material is provided over at least some of the discrete portions. Heating the discrete portions of reducible mixture to 1425 °C or 1400 °C or 1375 °C results in formation of an intermediate product of metallic iron nuggets and slag, and one or more metallic iron nuggets. The intermediate product with less than 5% mass MgO in the slag may have the ratio of percent by weight sulfur in the slag over percent sulfur in the metallic nuggets of at least about 12 or at least about 15. The metallic iron nuggets may have a sulfur content of less than 0.03%.
摘要:
A battery of stationary hearth furnaces, and method for using, for producing metallic iron nodules having a furnace having a stationary hearth, an inlet and an outlet; a heating chamber beneath the stationary hearth having heated fluids circulated thereto and heating reducible material on the stationary hearth; passageways circulating fluids, through ports from the furnace housing above the reducible material to the heating chamber beneath; burners and air inlets in the furnace and optionally in at least one passageway and a heating chamber for drying and heating the reducible material, driving off and burning volatile material, and forming metallic iron nodules; a loading device for loading reducible material and optionally hearth material onto the stationary hearth through the inlet; and a discharging device capable of discharging metallic iron nodules and optionally related material from the stationary hearth through the outlet.
摘要:
Method and system for producing metallic nuggets includes providing reducible mixture of reducing material (such as carbonaceous material) and reducible iron bearing material (such as iron oxide) arranged in discrete portions, such as mounds or briquettes, on at least a portion of a hearth material layer (such as carbonaceous material). A coarse overlayer of carbonaceous material is provided over at least some of the discrete portions. Heating the discrete portions of reducible mixture to 1425 °C or 1400 °C or 1375 °C results in formation of an intermediate product of metallic iron nuggets and slag, and one or more metallic iron nuggets. The intermediate product with less than 5% mass MgO in the slag may have the ratio of percent by weight sulfur in the slag over percent sulfur in the metallic nuggets of at least about 12 or at least about 15. The metallic iron nuggets may have a sulfur content of less than 0.03%.