A PROCESS FOR MAKING A LIGHTWEIGHT, CEMENTITIOUS, THREE-DIMENSIONAL STRUCTURE
    2.
    发明公开
    A PROCESS FOR MAKING A LIGHTWEIGHT, CEMENTITIOUS, THREE-DIMENSIONAL STRUCTURE 失效
    德国维多利亚州立大学维多利亚州立大学

    公开(公告)号:EP0814946A4

    公开(公告)日:1998-12-02

    申请号:EP96909688

    申请日:1996-03-13

    申请人: THERMOFLEX INC

    摘要: A process of making a light weight, cementitious, three-dimensional structure such as a building panel which includes the steps of measuring a quantity of water, measuring about 425 kilograms of cement, and between approximately 40 to 60 grams of ferric chloride in 40 % solution by volume per approximately 278 liters of said water, mixing said quantity of water, said cement and said ferric chloride, measuring between approximately .620 kilograms and 1 347 kilograms of substantially pure powdered aluminum, between approximately .230 kilograms and .710 kilograms of Hexafluorosilicate, between approximately .560 and .680 kilograms of calcium formate, and between approximately 4 and 8 kilograms of fiber, per approximately 278 liters of said water, combining said mixture of said cement, said ferric chloride and said water with said powdered aluminum, said Hexaflurosilicate, said calcium formate and said fiber, mixing said combination, waiting until said mixed combination rises, and forming the lightweight, cementitious, three-dimensional structure.

    摘要翻译: 本发明涉及一种制造重量轻的水泥质三维结构如建筑面板的方法,该方法包括以下步骤:测量约425千克水泥的水量和约40至60克氯化铁 在约278升水中以体积计40%溶液,将水,水泥和氯化铁的量混合在约0.620千克至1.347千克的基本上纯的铝粉之间,约0.230千克至0.710千克六氟硅酸盐之间, 约0.560至0.680千克的甲酸钙之间,约4至8千克纤维之间,每278升水,将水泥,氯化铁和水的混合物与粉末状铝,六氟硅酸盐,钙 甲酸和纤维,混合组合,等待混合组合升高,f 轻量化,水泥质的三维结构。