METHOD FOR PRODUCING SUPERCONDUCTING RADIO-FREQUENCY ACCELERATION CAVITY
    2.
    发明公开
    METHOD FOR PRODUCING SUPERCONDUCTING RADIO-FREQUENCY ACCELERATION CAVITY 审中-公开
    VERFAHREN ZUR HERSTELLUNG EINES SUPRALEITER-FUNKFREQUENZ-BESCHLEUNIGUNGSRAUMS

    公开(公告)号:EP2312915A1

    公开(公告)日:2011-04-20

    申请号:EP09804824.2

    申请日:2009-06-24

    IPC分类号: H05H7/20 C22B9/22 C22B34/24

    摘要: To provide a manufacturing method of a superconducting radio-frequency acceleration cavity used in a charged particle accelerator enabling the manufacturing with few waste amounts of the niobium material at low cost in a short time, the manufacturing method has each of the steps of (a) obtaining an ingot made from a disk-shaped niobium material, (b) slicing and cutting the niobium ingot into a plurality of niobium plates each with a predetermined thickness, by vibrating multiple wires back and forth while spraying fine floating abrasive grains with the niobium ingot supported, (c) removing the floating abrasive grains adhered to the sliced niobium plates, and (d) performing deep draw forming on the niobium plates and thereby obtaining a niobium cell of a desired shape.

    摘要翻译: 为了提供一种用于带电粒子加速器的超导射频加速腔的制造方法,其能够在短时间内以低成本制造少量的铌材料,所以制造方法具有以下步骤:(a) 获得由盘状铌材料制成的铸锭,(b)将铌锭切割并切割成具有预定厚度的多个铌板,通过在铌锭中喷洒细的浮动磨料颗粒来回振动多根钢丝 (c)去除附着在切片铌板上的浮动磨粒,(d)在铌板上进行深冲压成形,从而得到所需形状的铌电池。