公开(公告)号:EP3492182A1
公开(公告)日:2019-06-05
申请号:EP17834386.9
申请日:2017-07-26
Applicant: AGC INC.
Inventor: SAITO Shun , TOYODA Mizuna , AIKAWA Masataka
IPC: B05D1/36 , B05D3/10 , B05D7/24 , C09D5/03 , C09D127/12 , C09D175/04
Abstract: To provide a process for producing a coated article, capable of producing a coated article having a coating film excellent in weather resistance, using a powder coating material.
A process for producing a coated article having a substrate, comprising:
applying a curable powder coating material containing a curable polymer containing no fluorine atom, a curing agent and a pigment to a surface of a substrate, to form a first coating layer composed of the curable powder coating material, then
applying a powder coating material containing a fluorinated polymer and containing no pigment to a surface of the first coating layer, to form a second coating layer composed of the powder coating material, and
heating the first coating layer and the second coating layer simultaneously to form a coating film on the surface of the substrate.-
2.
公开(公告)号:EP3409737A1
公开(公告)日:2018-12-05
申请号:EP17744071.6
申请日:2017-01-19
Applicant: AGC INC.
Inventor: SAITO Shun , AIKAWA Masataka
IPC: C09D201/04 , B32B27/20 , B32B27/30 , C09D5/03 , C09D7/12 , C09D201/06
Abstract: To provide a powder coating material capable of forming a coating film that is excellent in weather resistance, processability and impact resistance and that improves corrosion resistance of a substrate (in particular, a substrate made of aluminum or of an aluminum alloy).
A powder coating material comprising a powder of a resin composition, wherein the resin composition comprises a fluorinated polymer (A) having a number average molecular weight of from 10,000 to 50,000 and a fluorine content of at least 10 mass%, a resin (B) having a fluorine content of less than 10 mass% or containing no fluorine atom, a curing agent, a plasticizer having a melting point of from 50 to 150°C and core-shell particles, and wherein the absolute value of the difference between the melting point of the plasticizer and the glass transition temperature of a polymer of a shell portion in the core-shell particles is within 30°C and the content of the plasticizer is from 5 to 25 parts by mass based on 100 parts by mass of the fluorinated polymer (A).-
公开(公告)号:EP3409737B1
公开(公告)日:2020-05-13
申请号:EP17744071.6
申请日:2017-01-19
Applicant: AGC INC.
Inventor: SAITO Shun , AIKAWA Masataka
IPC: C09D201/04 , B32B27/20 , B32B27/30 , C09D5/03 , C09D7/40 , C09D201/06 , C09D7/63 , C09D7/65 , C09D127/12 , C08F214/18 , C08F259/08 , C09D151/00 , C09D175/04 , C08F214/24 , C08L51/00
-
-