FIRE PROOF TREATMENT SOLUTION AND FIRE RETARDANT MATERIAL THEREFROM
    1.
    发明公开
    FIRE PROOF TREATMENT SOLUTION AND FIRE RETARDANT MATERIAL THEREFROM 有权
    FLAMMSCHUTZBEHANDLUNGSL SUNG UND FLAMMHEMMENDED MATERIAL DAVON

    公开(公告)号:EP1547739A4

    公开(公告)日:2005-06-29

    申请号:EP03733219

    申请日:2003-05-30

    摘要: A fire proof treatment solution capable of resolving problems, such as low solubility leading to low concentration and hence low combustion inhibiting effect and water solubility leading to a disadvantage of eluviation, of boron compounds used as a constituent of flame retarding treatment solution. In particular, a fire proof treatment solution produced by adding phosphoric acid and a silane coupling agent to a weak acid or weak alkali aqueous metal salt solution containing a boron compound to thereby obtain a mixed aqueous solution and adding a plant extract composed mainly of a polyphenol compound to the mixed aqueous solution. This fire proof treatment solution can be widely applied to members composed mainly of cellulose, such as wood, paper and natural fibers. This fire proof treatment solution can increase the fixation of chemicals to thereby attain a high combustion inhibiting effect and can minimize the occurrence of eluviation.

    摘要翻译: 本发明提供一种耐火处理液,其能够解决作为阻燃处理液的构成成分使用的硼化合物的低溶解性,低浓度化,低燃烧抑制效果,水溶解性等导致不易溶出的问题。 特别是在含有硼化合物的弱酸性或弱碱性金属盐水溶液中添加磷酸和硅烷偶联剂,得到混合水溶液,添加以多酚为主体的植物提取物的防火处理液 化合物混合到混合水溶液中。 这种防火处理溶液可广泛应用于主要由纤维素构成的构件,如木材,纸张和天然纤维。 这种防火处理溶液可以增加化学物质的固定,从而获得高的燃烧抑制效果,并且可以最小化淋溶的发生。

    METHOD OF MANUFACTURING NONCOMBUSTIBLE WOOD
    2.
    发明公开
    METHOD OF MANUFACTURING NONCOMBUSTIBLE WOOD 有权
    用于生产不燃木

    公开(公告)号:EP1452286A4

    公开(公告)日:2005-04-20

    申请号:EP02780111

    申请日:2002-11-15

    摘要: A method of manufacturing noncombustible wood capable of maximizing the amount of noncombustible agent used to impregnate the wood therewith, completely fulfilling the requirements of the Building Standard Law for noncombustible wood, and being manufactured rather easily, comprising three times of drying steps for drying the wood (for example, board material B), two times of decompressing steps for decompressing the wood, two times of decompressed impregnation steps for impregnating the wood with noncombustible treatment agent in decompressed state, and two times of pressurized impregnation steps for impregnating the wood with the noncombustible treatment agent in pressurized state.