An improved fiber reinforced glass composite includes a boron nitride-coated refractory fiber in a matrix of a black glass ceramic having the empirical formula SiCxOy where x ranges from about 0.5 to about 2.0, preferably 0.9 to 1.6 and y ranges from about 0.5 to 3.0, preferably 0.7 to 1.8. Preferably the black glass ceramic is derived from cyclosiloxane monomers containing a vinyl group attached to silicon and/or a hydride-silicon group. Graceful failure can be obtained after exposure of the composites to temperatures up to 600-700 °C in air.
摘要:
An improved fiber reinforced glass composite includes a refractory fiber in a matrix of a nitrogen-containing black glass ceramic having the empirical formula SiNzCxOy where x ranges from greater than zero up to about 2.0, preferably 0.1 to 1.0, y ranges from 0.5 up to about 3.0, preferably 0.7 to 1.8, and z ranges from above zero up to about 1.5, preferably 0.2 to 1.0. Preferably the black glass ceramic is derived from cyclosiloxane monomers containing a vinyl group attached to silicon and/or a hydride-silicon group. The cyclosiloxane monomers are polymerized and then pyrolyzed in an ammonia-containing atmosphere to produce the nitrogen-containing black glass (silicon oxycarbonitride).
摘要:
An improved protective layer for ceramic insulating bodies comprises a composite having a refractory fiber in a matrix of a black glass ceramic having the empirical formula SiCxOy where x ranges from about 0.5 to about 2.0, preferably 0.9 to 1.6 and y ranges from about 0.5 to 3.0, preferably 0.7 to 1.8. The black glass ceramic is derived from cyclosiloxane monomers containing a vinyl group attached to silicon and/or a hydride-silicon group.
摘要:
An improved fiber reinforced glass composite includes a boron nitride-coated refractory fiber in a matrix of a black glass ceramic having the empirical formula SiCxOy where x ranges from about 0.5 to about 2.0, preferably 0.9 to 1.6 and y ranges from about 0.5 to 3.0, preferably 0.7 to 1.8. Preferably the black glass ceramic is derived from cyclosiloxane monomers containing a vinyl group attached to silicon and/or a hydride-silicon group. Graceful failure can be obtained after exposure of the composites to temperatures up to 600-700 °C in air.
摘要:
An improved fiber reinforced glass composite includes a refractory fiber in a matrix of a nitrogen-containing black glass ceramic having the empirical formula SiNzCxOy where x ranges from greater than zero up to about 2.0, preferably 0.1 to 1.0, y ranges from 0.5 up to about 3.0, preferably 0.7 to 1.8, and z ranges from above zero up to about 1.5, preferably 0.2 to 1.0. Preferably the black glass ceramic is derived from cyclosiloxane monomers containing a vinyl group attached to silicon and/or a hydride-silicon group. The cyclosiloxane monomers are polymerized and then pyrolyzed in an ammonia-containing atmosphere to produce the nitrogen-containing black glass (silicon oxycarbonitride).
摘要:
A black glass having the empirical formula SiCxOy where x is greater than zero and up to about 2.0 and y is greater than zero and up to about 2.2 is produced from a cyclosiloxane polymer precursor by pyrolysis in the presence of oxygen by heating at a rate exceeding about 5 °C/min.
摘要:
A protective layer for polymeric composite substrates comprises a fiber-reinforced glass composite having a refractory fiber in a matrix of a black glass ceramic having the empirical formula SiCxOy where x ranges from about 0.5 to about 2.0, preferably 0.9 to 1.6 and y ranges from about 0.5 to 3.0, preferably 0.7 to 1.8. The black glass ceramic is derived from cyclosiloxane monomers containing a vinyl group attached to silicon and/or a hydride-silicon group.
摘要:
A protective layer for polymeric composite substrates comprises a fiber-reinforced glass composite having a refractory fiber in a matrix of a black glass ceramic having the empirical formula SiCxOy where x ranges from about 0.5 to about 2.0, preferably 0.9 to 1.6 and y ranges from about 0.5 to 3.0, preferably 0.7 to 1.8. The black glass ceramic is derived from cyclosiloxane monomers containing a vinyl group attached to silicon and/or a hydride-silicon group.
摘要:
An improved fiber reinforced glass composite includes a boron nitride-coated refractory fiber in a matrix of a black glass ceramic having the empirical formula SiCxOy where x ranges from about 0.5 to about 2.0, preferably 0.9 to 1.6 and y ranges from about 0.5 to 3.0, preferably 0.7 to 1.8. Preferably the black glass ceramic is derived from cyclosiloxane monomers containing a vinyl group attached to silicon and/or a hydride-silicon group. Graceful failure can be obtained after exposure of the composites to temperatures up to 600-700 °C in air.
摘要:
An improved protective layer for ceramic insulating bodies comprises a composite having a refractory fiber in a matrix of a black glass ceramic having the empirical formula SiCxOy where x ranges from about 0.5 to about 2.0, preferably 0.9 to 1.6 and y ranges from about 0.5 to 3.0, preferably 0.7 to 1.8. The black glass ceramic is derived from cyclosiloxane monomers containing a vinyl group attached to silicon and/or a hydride-silicon group.