    摘要: According to the invention, an iron oxide is provided for ferrite having a Mn content of 0,1 to 0,3 % by weight and a P content of not more than 0,005 % by weight. Such an iron oxide can easily be produced by making an iron chloride solution, dephosphorizing the iron chloride solution by a simple process and oxidizing roasting the dephosphorized solution to provide the desired iron oxide. Although Mn is contained as an impurity the ferrite properties are not impaired thereby since attention is paid to the impurities of P which are at a low level. Accordingly, soft ferrite can be produced having excellent ferrite properties.

    摘要翻译: 根据本发明,提供了一种氧化铁,其铁含量为Mn含量为0.1至0.3重量%,P含量不超过0.005重量%。 这样的氧化铁可以容易地通过制造氯化铁溶液来制造,通过简单的方法对氯化铁溶液进行脱磷,并对脱磷酸溶液进行氧化焙烧以提供所需的氧化铁。 虽然含有Mn作为杂质,但由于注意处于低水平的P的杂质,铁素体的性质不会受到损害。 因此,可以制造铁氧体性质优异的软铁氧体。

    Iron oxide for ferrite
    2.
    发明公开
    Iron oxide for ferrite 失效
    铁矿氧化铁

    公开(公告)号:EP0343283A3

    公开(公告)日:1990-06-20

    申请号:EP88121025.6

    申请日:1988-12-15

    IPC分类号: C01G49/06

    摘要: According to the invention, an iron oxide is provided for ferrite having a Mn content of 0,1 to 0,3 % by weight and a P content of not more than 0,005 % by weight. Such an iron oxide can easily be produced by making an iron chloride solution, dephosphorizing the iron chloride solution by a simple process and oxidizing roasting the dephosphorized solution to provide the desired iron oxide. Although Mn is contained as an impurity the ferrite properties are not impaired thereby since attention is paid to the impurities of P which are at a low level. Accordingly, soft ferrite can be produced having excellent ferrite properties.

    Purified solution containing iron and manganese, and method producing thereof
    3.
    发明公开
    Purified solution containing iron and manganese, and method producing thereof 失效
    含有它们的制备铁和锰,并且过程纯化的溶液。

    公开(公告)号:EP0364904A2

    公开(公告)日:1990-04-25

    申请号:EP89119089.4

    申请日:1989-10-13

    IPC分类号: C01G49/00 C22B47/00

    摘要: A solution containing iron chloride and manganese chloride, whose phosphorus content is not higher than 0.007 wt.% with respect to the total content of iron and manganese. A method for producing the said solution comprises the steps of dissolving manganese containing raw material in hydrochloric solution; oxidizing the solution; adjusting the pH of the solution to 2.5 ∼ 4.5; separating the insolubles from the solution. This solution can be utilized to produce a mixed powder of an iron oxide and a manganese oxide. And the mixed powder is useful for producing a high-quality soft ferrite.