PEELABLE BUFFER LAYER HAVING A PREFERENTIAL TEAR PORTION AND METHODS OF MANUFACTURING THE SAME
    3.
    发明公开
    PEELABLE BUFFER LAYER HAVING A PREFERENTIAL TEAR PORTION AND METHODS OF MANUFACTURING THE SAME 审中-公开
    根据上述制造偏好内容的一部分并且处理免赔额缓冲层

    公开(公告)号:EP1556725A1

    公开(公告)日:2005-07-27

    申请号:EP03774813.4

    申请日:2003-10-14

    IPC分类号: G02B6/44

    CPC分类号: G02B6/4495 G02B6/4402

    摘要: A tight buffered optical fiber (10) and methods of manufacturing the same include an optical fiber (1) and a tight buffer layer (15). The tight buffer layer has a predetermined wall thickness (t) generally surrounding the optical fiber and at least one preferential tear portion generally formed along a longitudinal axis of the tight buffer layer. In one embodiment, the tight buffered optical fiber has a delta attenuation of about 0.300 dB/km or less at a temperature of about -40 °C at a reference wavelength of about 1550 nm, thereby making the tight buffered optical fiber suitable for outdoor environments. Other embodiments can include a buffer layer surrounding one or more optical fiber ribbons. In other embodiments, the buffer layer can be formed from a material having an elongation to break ratio of about 500% or less.