公开(公告)号:EP2484727A1
公开(公告)日:2012-08-08
申请号:EP10820632.7
申请日:2010-09-30
发明人: SHIODA, Satoshi , ISHITOBI, Tatsuro , OTOMARU, Takao , MATSUO, Rumiko , MIYATA, Eiichi , INUMARU, Masaki , SUGITA, Yukio , YAMAZAKI, Fumie , SHIRAISHI, Naoki , TAMURA, Mitsuyoshi
CPC分类号: C09D11/322 , B82Y30/00 , C01P2004/62 , C01P2004/64 , C09C1/56 , C09D11/324 , Y10T428/24802
摘要: A main object of the present invention is to provide an ink composition which has superior storage stability, is resistant to bleeding, and has good fixability to paper, enables printing of a clear image. In the present invention, the above objecct can be attained by providing an ink composition comprising a pigment dispersion containing a surface-treated pigment and a resin emulsion, wherein: the surface-treated pigment is obtained by binding a functional group, having a larger calcium index than a calcium index of 1, 2, 3-benzenetricarboxylic acid, to the surface of a pigment; and the resin emulsion is adapted so that an aqueous solution containing 1 mass % of a solid content of the resin emulsion has a conductance of 300 µS/cm or less.
摘要翻译: 本发明的主要目的在于提供具有优异的保存稳定性,耐渗色性,对纸张的定影性良好,能够印刷清晰的图像的油墨组合物。 在本发明中,通过提供包含含有表面处理过的颜料和树脂乳液的颜料分散体的油墨组合物可获得上述目的,其中:表面处理过的颜料是通过将具有较大钙的官能团 指数比1,2,3-苯三甲酸的钙指数高的指数到颜料的表面; 并且树脂乳液适合使得包含1质量%树脂乳液的固体内容物的水溶液具有300μS/ cm或更小的电导率。
-
公开(公告)号:EP2660066A1
公开(公告)日:2013-11-06
申请号:EP11852489.1
申请日:2011-12-26
发明人: INUMARU, Masaki , SHIODA, Satoshi , MIYATA, Eiichi , OTOMARU, Takao , SUGITA, Yukio , TAMURA, Mitsuyoshi , YAMAZAKI, Fumie , SHIRAISHI, Naoki
CPC分类号: B41M5/0017 , C09D11/322 , C09D11/54
摘要: An inkjet recording method which suppresses feathering and color bleeding and is excellent in fixability to a recording medium. The inkjet recording method comprises the steps off:
applying an ink-receiving solution prepared by dissolving in an aqueous solvent at least one metal salt having a water solubility of 0.1 mol/l or more, selected from calcium salts, magnesium salts, nickel salts and zinc salts having a valence of 2 or more, to at least the surface to be printed by using an inkjet ink or the entire surface of a recording medium; and
printing on the metal salt adhered part by using the inkjet ink comprising at least a pigment, a resin emulsion and an aqueous solvent containing a surfactant, wherein
a phosphorus-containing group having at least one P-O or P=O bond is bound to the surface of the pigment.摘要翻译: 一种喷墨记录方法,其抑制羽化和褪色,并且对记录介质的定影性优异。 所述喷墨记录方法包括以下步骤:将通过溶解在水性溶剂中制备的至少一种水溶性为0.1mol / l或更高的选自钙盐,镁盐,镍盐和 通过使用喷墨油墨或记录介质的整个表面,至少在要印刷的表面上形成具有2或更高价的锌盐; 并且通过使用包含至少一种颜料,树脂乳液和含有表面活性剂的含水溶剂的喷墨油墨在金属盐粘附部分上印刷,其中含有至少一个PO或P = O键的含磷基团与 颜料表面。
-
公开(公告)号:EP2660066B1
公开(公告)日:2016-04-20
申请号:EP11852489.1
申请日:2011-12-26
发明人: INUMARU, Masaki , SHIODA, Satoshi , MIYATA, Eiichi , OTOMARU, Takao , SUGITA, Yukio , TAMURA, Mitsuyoshi , YAMAZAKI, Fumie , SHIRAISHI, Naoki
CPC分类号: B41M5/0017 , C09D11/322 , C09D11/54
-
公开(公告)号:EP3804981A1
公开(公告)日:2021-04-14
申请号:EP19815113.6
申请日:2019-06-05
发明人: SHIODA, Satoshi , KANETAKA, Hidenari , KONISHI, Kenta , SAWADA, Masanori , SHIOTA, Ryunosuke , KISHIMOTO, Yoshihiro , OKANO, Ai
摘要: Provided is a barrier film which is less likely to undergo deterioration of gas barrier properties even after the Gelbo Flex test. The barrier film according to the present invention includes a barrier coat layer, an inorganic oxide vapor deposition layer, and a substrate layer in this order, the barrier coat layer being a cured film of a barrier coat composition containing: a hydrolyzed product of an alkoxysilane represented by the following General Formula (I): Si(OR 1 ) 4 ... (I), wherein R 1 represents an organic functional group; a water-soluble polymer; and a hydrolyzed product of a silane coupling agent represented by the following General Formula (II): R 2 n Si(OR 3 ) 4-n ... (II), wherein R 2 and R 3 each independently represent an organic functional group, and n is 2 or 3.
-
-
-