SINGLE STAGE DRAWING FOR MPD-I YARNS
    1.
    发明公开
    SINGLE STAGE DRAWING FOR MPD-I YARNS 有权
    MPD-I纱线的单阶段图纸

    公开(公告)号:EP2235242A1

    公开(公告)日:2010-10-06

    申请号:EP08867787.7

    申请日:2008-12-18

    IPC分类号: D01F6/60 D01D5/04

    摘要: The invention relates to a continuous dry spinning process for preparing a fiber from a polymer solution having concentrations of polymer, salt, solvent and water. After the fiber is extruded and quenched, the fiber is placed in contact with a conditioning solution comprising concentrations of solvent, salt, and water. The conditioning solution acts upon the fiber to plasticize the fiber prior to being drawn. The conditioning solution has concentrations of solvent, salt, and water so that the fiber is plasticized to the extent necessary for drawing but does not plasticize the fiber to such an extent as to re-dissolve the fiber into a polymeric solution. A heat-treated fiber manufactured from this process has improved shrinkage and can be colored to darker shades.

    摘要翻译: 本发明涉及由具有聚合物,盐,溶剂和水的浓度的聚合物溶液制备纤维的连续干纺工艺。 在纤维被挤出并淬火后,将纤维与包含溶剂,盐和水的浓度的调节溶液接触。 调理溶液在被拉伸之前作用于纤维以塑化纤维。 调理溶液具有溶剂,盐和水的浓度,使得纤维塑化至拉伸所需的程度,但不使纤维增塑至将纤维重新溶解成聚合物溶液的程度。 由该工艺制造的热处理纤维具有改善的收缩率,并可着色成较暗的色调。

    RAPID PLASTICIZATION OF QUENCHED YARNS
    2.
    发明授权
    RAPID PLASTICIZATION OF QUENCHED YARNS 有权
    FAST塑化淬火YARN

    公开(公告)号:EP2222905B1

    公开(公告)日:2011-10-26

    申请号:EP08863364.9

    申请日:2008-12-18

    IPC分类号: D01D5/04 D01F6/60

    摘要: The invention relates to a continuous dry spinning process for preparing a fiber from a polymer solution having concentrations of polymer, salt, solvent and water. After the fiber is extruded and quenched, the fiber is placed in contact with a conditioning solution comprising concentrations of solvent, salt, and water. The conditioning solution acts upon the fiber to plasticize the fiber prior to being drawn. The conditioning solution has concentrations of solvent, salt, and water so that the fiber is plasticized to the extent necessary for drawing but does not plasticize the fiber to such an extent as to re-dissolve the fiber into a polymeric solution. A heat-treated fiber manufactured from this process has improved shrinkage and can be colored to darker shades.

    HIGH-SPEED META-ARAMID FIBER PRODUCTION
    4.
    发明公开
    HIGH-SPEED META-ARAMID FIBER PRODUCTION 有权
    HIGH-SPEED间位芳纶纤维生产

    公开(公告)号:EP2231905A1

    公开(公告)日:2010-09-29

    申请号:EP08862329.3

    申请日:2008-12-18

    IPC分类号: D01D5/04

    CPC分类号: D01D5/04 D01F6/605

    摘要: The invention relates to a continuous dry spinning process for preparing a fiber from a polymer solution having concentrations of polymer, salt, solvent and water. After the fiber is extruded and quenched, the fiber is placed in contact with a conditioning solution comprising concentrations of solvent, salt, and water. The conditioning solution acts upon the fiber to plasticize the fiber prior to being drawn. The conditioning solution has concentrations of solvent, salt, and water so that the fiber is plasticized to the extent necessary for drawing but does not plasticize the fiber to such an extent as to re-dissolve the fiber into a polymeric solution. A heat-treated fiber manufactured from this process has improved shrinkage and can be colored to darker shades.

    MULTISTAGE DRAW WITH RELAXATION STEP
    6.
    发明公开
    MULTISTAGE DRAW WITH RELAXATION STEP 有权
    MEHRSTUFIGE ZUGSPANNUNG MIT ENTSPANNUNGSSTUFE

    公开(公告)号:EP2235241A1

    公开(公告)日:2010-10-06

    申请号:EP08866870.2

    申请日:2008-12-18

    IPC分类号: D01F6/60 D01D5/04

    摘要: The invention relates to a continuous dry spinning process for preparing a fiber from a polymer solution having concentrations of polymer, salt, solvent and water. After the fiber is extruded and quenched, the fiber is placed in contact with a conditioning solution comprising concentrations of solvent, salt, and water. The conditioning solution acts upon the fiber to plasticize the fiber prior to being drawn. The conditioning solution has concentrations of solvent, salt, and water so that the fiber is plasticized to the extent necessary for drawing but does not plasticize the fiber to such an extent as to re-dissolve the fiber into a polymeric solution. A heat-treated fiber manufactured from this process has improved shrinkage and can be colored to darker shades.

    摘要翻译: 本发明涉及一种从具有聚合物,盐,溶剂和水的浓度的聚合物溶液制备纤维的连续干法纺丝方法。 纤维被挤出和淬火后,将纤维置于与包含溶剂,盐和水的浓度的调理溶液接触。 调理溶液作用于纤维,以在拉伸之前使纤维增塑。 调理溶液具有溶剂,盐和水的浓度,使得纤维被塑化至拉伸所需的程度,但不会使纤维增塑至使纤维再溶解成聚合物溶液的程度。 由该方法制造的经热处理的纤维具有改善的收缩率并且可以着色到较暗的色调。

    LOW SHRINKAGE, DYEABLE MPD-I YARN
    7.
    发明公开
    LOW SHRINKAGE, DYEABLE MPD-I YARN 有权
    可染热收缩ARM MPD-I YARN

    公开(公告)号:EP2222904A1

    公开(公告)日:2010-09-01

    申请号:EP08863119.7

    申请日:2008-12-18

    摘要: The invention relates to a continuous dry spinning process for preparing a fiber from a polymer solution having concentrations of polymer, salt, solvent and water. After the fiber is extruded and quenched, the fiber is placed in contact with a conditioning solution comprising concentrations of solvent, salt, and water. The conditioning solution acts upon the fiber to plasticize the fiber prior to being drawn. The conditioning solution has concentrations of solvent, salt, and water so that the fiber is plasticized to the extent necessary for drawing but does not plasticize the fiber to such an extent as to re-dissolve the fiber into a polymeric solution. A heat-treated fiber manufactured from this process has improved shrinkage and can be colored to darker shades.

    HIGH-SPEED META-ARAMID FIBER PRODUCTION
    8.
    发明授权
    HIGH-SPEED META-ARAMID FIBER PRODUCTION 有权
    HIGH-SPEED间位芳纶纤维生产

    公开(公告)号:EP2231905B1

    公开(公告)日:2011-11-09

    申请号:EP08862329.3

    申请日:2008-12-18

    IPC分类号: D01D5/04

    CPC分类号: D01D5/04 D01F6/605

    摘要: The invention relates to a continuous dry spinning process for preparing a fiber from a polymer solution having concentrations of polymer, salt, solvent and water. After the fiber is extruded and quenched, the fiber is placed in contact with a conditioning solution comprising concentrations of solvent, salt, and water. The conditioning solution acts upon the fiber to plasticize the fiber prior to being drawn. The conditioning solution has concentrations of solvent, salt, and water so that the fiber is plasticized to the extent necessary for drawing but does not plasticize the fiber to such an extent as to re-dissolve the fiber into a polymeric solution. A heat-treated fiber manufactured from this process has improved shrinkage and can be colored to darker shades.

    LOW SHRINKAGE, DYEABLE MPD-I YARN
    9.
    发明授权
    LOW SHRINKAGE, DYEABLE MPD-I YARN 有权
    可染热收缩ARM MPD-I YARN

    公开(公告)号:EP2222904B1

    公开(公告)日:2011-10-26

    申请号:EP08863119.7

    申请日:2008-12-18

    摘要: The invention relates to a continuous dry spinning process for preparing a fiber from a polymer solution having concentrations of polymer, salt, solvent and water. After the fiber is extruded and quenched, the fiber is placed in contact with a conditioning solution comprising concentrations of solvent, salt, and water. The conditioning solution acts upon the fiber to plasticize the fiber prior to being drawn. The conditioning solution has concentrations of solvent, salt, and water so that the fiber is plasticized to the extent necessary for drawing but does not plasticize the fiber to such an extent as to re-dissolve the fiber into a polymeric solution. A heat-treated fiber manufactured from this process has improved shrinkage and can be colored to darker shades.

    RAPID PLASTICIZATION OF QUENCHED YARNS
    10.
    发明公开
    RAPID PLASTICIZATION OF QUENCHED YARNS 有权
    FAST塑化淬火YARN

    公开(公告)号:EP2222905A1

    公开(公告)日:2010-09-01

    申请号:EP08863364.9

    申请日:2008-12-18

    IPC分类号: D01D5/04 D01F6/60

    摘要: The invention relates to a continuous dry spinning process for preparing a fiber from a polymer solution having concentrations of polymer, salt, solvent and water. After the fiber is extruded and quenched, the fiber is placed in contact with a conditioning solution comprising concentrations of solvent, salt, and water. The conditioning solution acts upon the fiber to plasticize the fiber prior to being drawn. The conditioning solution has concentrations of solvent, salt, and water so that the fiber is plasticized to the extent necessary for drawing but does not plasticize the fiber to such an extent as to re-dissolve the fiber into a polymeric solution. A heat-treated fiber manufactured from this process has improved shrinkage and can be colored to darker shades.