公开(公告)号:EP1234837B1
公开(公告)日:2005-09-07
申请号:EP02075520.3
申请日:2002-02-11
发明人: Gauthier, William J. , Lopez, Margarito , Rauscher, David J. , Campbell, Donald G., Jr. , Kerr, Margaret Elaine
IPC分类号: C08F10/00
CPC分类号: C08F10/00 , C08F4/65904 , C08F4/65912 , C08F4/65927 , C08F110/06 , C08F4/65916 , C08F2500/16 , C08F2500/18 , C08F2500/12 , C08F2500/03 , C08F2500/15
-
公开(公告)号:EP1234837A1
公开(公告)日:2002-08-28
申请号:EP02075520.3
申请日:2002-02-11
发明人: Gauthier, William J. , Lopez, Margarito , Rauscher, David J. , Campbell, Donald G., Jr. , Kerr, Margaret Elaine
IPC分类号: C08F10/00
CPC分类号: C08F10/00 , C08F4/65904 , C08F4/65912 , C08F4/65927 , C08F110/06 , C08F4/65916 , C08F2500/16 , C08F2500/18 , C08F2500/12 , C08F2500/03 , C08F2500/15
摘要: Process of preparing silica-supported catalysts. A support material comprising silica particles impregnated with an alumoxane co-catalyst with at least one-half of the co-catalyst disposed within the internal pore volume of the silica is contacted with a dispersion of a metallocene catalyst in an aromatic solvent. The dispersion and support are mixed at a temperature of about 10°C or less to enable the metallocene to become reactively supported on and impregnated within the alumoxane-impregnated silica particles. The supported catalyst is recovered from the aromatic solvent and washed with an aromatic hydrocarbon and then a paraffinic hydrocarbon at a temperature of about 10°C or less. The washed catalyst is dispersed in a viscous mineral oil.
摘要翻译: 制备二氧化硅负载型催化剂的方法。 包含用铝氧烷助催化剂浸渍的二氧化硅颗粒与载体在二氧化硅的内孔体积内的至少一半助催化剂的载体材料与金属茂催化剂在芳族溶剂中的分散体接触。 分散体和载体在约10℃或更低的温度下混合以使茂金属能够反应性负载并浸渍在铝氧烷浸渍的二氧化硅颗粒内。 从芳香族溶剂中回收负载型催化剂,并在约10℃或更低的温度下用芳烃然后用链烷烃洗涤。 洗过的催化剂分散在粘稠的矿物油中。
-