公开(公告)号:EP1238000B1
公开(公告)日:2003-09-03
申请号:EP00993321.9
申请日:2000-11-22
CPC分类号: C08L15/00 , C08C19/06 , C08K3/08 , C08K3/10 , C08K3/11 , C08K3/22 , C08L9/02 , C08L9/06 , C08L21/00 , C08L23/283 , G10K11/165 , Y10T428/31696 , Y10T428/31707 , Y10T428/31855 , C08L2666/08 , C08L2666/04 , C08L2666/02
摘要: The invention relates to a rubber-based soundproofing material. The vulcanised rubber mixture consists of the following components: - a rubber or rubber blend; -a heavy metal and/or its alloys and/or its oxides and/or its salts in powder form, in addition to conventional mixing ingredients. The inventive material is characterised by a rubber mixture based on non-blended chlorobutyl rubber, bromobutyl rubber or acrylate rubber; or nitrile rubber or styrene-butadiene rubber, both of which are blended with epoxidised natural rubber. The rubber mixture has the following proportions: 10-50 wt. % rubber or rubber blend, 85-40 wt. % heavy metal and/or its alloys and/or its oxides and/or its salts, 5-10 wt. % mixing ingredients. The inventive rubber material based on bromobutyl rubber and Fe powder (curves a and b) is compared with sheet metal (curves c and d).
-
公开(公告)号:EP1238000A1
公开(公告)日:2002-09-11
申请号:EP00993321.9
申请日:2000-11-22
CPC分类号: C08L15/00 , C08C19/06 , C08K3/08 , C08K3/10 , C08K3/11 , C08K3/22 , C08L9/02 , C08L9/06 , C08L21/00 , C08L23/283 , G10K11/165 , Y10T428/31696 , Y10T428/31707 , Y10T428/31855 , C08L2666/08 , C08L2666/04 , C08L2666/02
摘要: The invention relates to a rubber-based soundproofing material. The vulcanised rubber mixture consists of the following components: - a rubber or rubber blend; -a heavy metal and/or its alloys and/or its oxides and/or its salts in powder form, in addition to conventional mixing ingredients. The inventive material is characterised by a rubber mixture based on non-blended chlorobutyl rubber, bromobutyl rubber or acrylate rubber; or nitrile rubber or styrene-butadiene rubber, both of which are blended with epoxidised natural rubber. The rubber mixture has the following proportions: 10-50 wt. % rubber or rubber blend, 85-40 wt. % heavy metal and/or its alloys and/or its oxides and/or its salts, 5-10 wt. % mixing ingredients. The inventive rubber material based on bromobutyl rubber and Fe powder (curves a and b) is compared with sheet metal (curves c and d).
-