OPTICAL PROCESSING STRUCTURE OF OPTICAL FIBER

    公开(公告)号:EP3933466A1

    公开(公告)日:2022-01-05

    申请号:EP20782315.4

    申请日:2020-03-25

    IPC分类号: G02B6/02 G02B6/44

    摘要: An optical processing structure of an optical fiber includes: an optical fiber that includes a core, a cladding, and a coating, the coating being partially removed; a thermally conductive protective material made of a silicone-based thermally conductive compound and provided around the cladding in a coating removed region of the optical fiber; and a thermally conductive base material on which the optical fiber is placed. The thermally conductive protective material contains a filler having a refractive index higher than that of the cladding. The filler is present in a region where evanescent light seeping out of the cladding is present when cladding mode light propagating in the cladding is totally reflected.

    MOLDED ARTICLE
    4.
    发明公开
    MOLDED ARTICLE 审中-公开

    公开(公告)号:EP3689973A1

    公开(公告)日:2020-08-05

    申请号:EP18863337.4

    申请日:2018-09-28

    摘要: The present invention relates to a molded article provided with a resin part formed with a thermoplastic resin composition capable of dispersing cellulose simply and uniformly in a highly hydrophobic resin and capable of improving the mechanical strength of a molded material formed using a resultant resin composition. The molded article is provided with a resin part formed with a thermoplastic resin composition containing 5 to 70 parts by mass of cellulose based on 100 parts by mass of the thermoplastic resin and containing an organic peroxide, wherein a tensile strength of a resin molded body formed with the thermoplastic resin composition measured in accordance with JIS K 7161 is 40 MPa or more.

    BIPOLAR STORAGE BATTERY
    8.
    发明公开

    公开(公告)号:EP4224570A1

    公开(公告)日:2023-08-09

    申请号:EP21875131.1

    申请日:2021-09-09

    摘要: Provided is a bipolar storage battery in which, even when growth occurs in a positive electrode due to corrosion caused by sulfuric acid contained in an electrolytic solution, the electrolytic solution is hard to penetrate into an interface between the positive electrode and an adhesive and battery performance is hard to decrease. The bipolar storage battery is a bipolar storage battery (1) including a bipolar electrode (130) including a positive electrode (120), a negative electrode (110), and a bipolar plate (111) in which the positive electrode (120) is provided on one surface and the negative electrode (110) is provided on the other surface, and the bipolar electrode (130) includes a covering member (150) configured to cover a peripheral part (120a) of an opposite surface of the positive electrode (120) in close contact with the peripheral part (120a), the opposite surface being opposite to a surface, of the positive electrode (120a), bonded to the bipolar plate (111).

    BIPOLAR LEAD-ACID BATTERY
    9.
    发明公开

    公开(公告)号:EP4224569A1

    公开(公告)日:2023-08-09

    申请号:EP21875093.3

    申请日:2021-09-06

    IPC分类号: H01M4/14 H01M4/68 H01M10/18

    摘要: Provided is a bipolar lead-acid battery in which the electrolyte is less likely to infiltrate into the interface between a positive electrode lead layer and an adhesive layer, deterioration in battery performance is less likely to occur. A positive electrode (120) of a bipolar electrode (130) of a bipolar lead-acid battery (1) includes a positive electrode lead layer (101) that is formed of lead or lead alloy and is disposed on one surface of a substrate (111), and an adhesive layer (140) that is disposed between the one surface of the substrate (111) and the positive electrode lead layer (101) and bonds the one surface of the substrate (111) and the positive electrode lead layer (101). The substrate (111) is formed of a thermoplastic resin, and the adhesive layer (140) is formed of a cured product of a reaction-curing type adhesive that is cured by reaction between a main agent containing an epoxy resin and a curing agent containing an amine compound. Even in a case where the adhesive layer (140) is immersed in a sulfuric acid with a concentration of 38% by mass at a temperature of 60°C for four weeks, the sulfuric acid does not infiltrate into the interface between the positive electrode lead layer (101) and the adhesive layer (140) .

    MOLDED ARTICLE
    10.
    发明公开
    MOLDED ARTICLE 审中-公开

    公开(公告)号:EP3705520A1

    公开(公告)日:2020-09-09

    申请号:EP18874930.3

    申请日:2018-10-31

    摘要: The present invention relates to a molded article provided with a resin part formed using a polyolefin resin composite material in which the size of an aggregate of cellulose is sufficiently small, and a highly hydrophobic polyolefin resin and the cellulose are integrated with a high degree of uniformity, the resin part having an improved mechanical strength.
    The molded article is provided with a resin part formed with a polyolefin resin composite material, the polyolefin resin composite material containing a polyolefin resin and 10 to 150 parts by mass of cellulose based on 100 parts by mass of the polyolefin resin, wherein an area of an aggregate of the cellulose is less than 20,000 µm 2 .