Process of preparing polyamine-epihalohydrin resins with reduced byproduct content
    1.
    发明公开
    Process of preparing polyamine-epihalohydrin resins with reduced byproduct content 有权
    制备副产物含量降低的聚胺 - 表卤代醇树脂的方法

    公开(公告)号:EP1770109A3

    公开(公告)日:2007-10-03

    申请号:EP07000112.8

    申请日:2000-06-12

    摘要: A process for rendering a polyamine-epihalohydrin resin storable stable, comprising: treating a composition containing a polyamine-epihalohydrin resin which includes CPD-forming species with at least one acidic agent, wherein the pH during treatment is about 1.1 or less; the time is for at least about 2 hours to at least about 24 hours, and the temperature is at least about 30 °C to at least about 90 °C, wherein the temperature range is combined with the time period range in an inverse relationship, to at least one of inhibit, reduce and remove the CPD-forming species to obtain a gelation storage stable reduced CPD-forming resin so that the composition containing the reduced CPD-forming polyamine-epihalohydrin resin, when stored at pH 1 for 24 hours at 50 °C and measured at 24 hours, produces less than about 500 ppm dry basis of CPD.

    摘要翻译: 一种使聚胺 - 表卤代醇树脂储存稳定的方法,包括:用至少一种酸性试剂处理含有包含CPD形成物质的聚胺 - 表卤代醇树脂的组合物,其中处理期间的pH值为约1.1或更小; 时间为至少约2小时至至少约24小时,并且温度为至少约30℃至至少约90℃,其中温度范围与时间范围以相反的关系相结合, 以抑制,还原和去除形成CPD的物质中的至少一种,以获得凝胶储存稳定减少的CPD形成树脂,使得当在pH 1下储存24小时时,含有形成CPD的减少的多胺 - 表卤代醇树脂的组合物 50°C,并在24小时测量,产生的CPD的干基数小于约500 ppm。

    Process of preparing polyamine-epihalohydrin resins with reduced byproduct content
    5.
    发明公开
    Process of preparing polyamine-epihalohydrin resins with reduced byproduct content 有权
    一种制备聚胺 - 表卤醇树脂与副产物含量降低过程

    公开(公告)号:EP1770109A2

    公开(公告)日:2007-04-04

    申请号:EP07000112.8

    申请日:2000-06-12

    摘要: A process for rendering a polyamine-epihalohydrin resin storable stable, comprising: treating a composition containing a polyamine-epihalohydrin resin which includes CPD-forming species with at least one acidic agent, wherein the pH during treatment is about 1.1 or less; the time is for at least about 2 hours to at least about 24 hours, and the temperature is at least about 30 °C to at least about 90 °C, wherein the temperature range is combined with the time period range in an inverse relationship, to at least one of inhibit, reduce and remove the CPD-forming species to obtain a gelation storage stable reduced CPD-forming resin so that the composition containing the reduced CPD-forming polyamine-epihalohydrin resin, when stored at pH 1 for 24 hours at 50 °C and measured at 24 hours, produces less than about 500 ppm dry basis of CPD.

    摘要翻译: 一种用于使聚胺 - 表卤醇树脂的方法可存储稳定,包括:治疗的组合物含有聚胺 - 表卤醇树脂其中包含CPD形成种类与至少一种酸性剂,治疗期间worin pH为约1.1或更小; 的时间为至少约2小时到至少约24小时,所述温度为至少约30℃到至少约90℃,worin的温度范围与时间段相结合的范围在反比关系, 为了抑制中的至少一个,还原除去该CPD形成种类,以获得凝胶化储存稳定降低CPD形成性树脂所以没有含还原CPD-形成聚胺 - 表卤醇树脂的组合物中,当存储在pH 1 24小时在 50℃,并在24小时测量,产生小于CPD的约500ppm干基。