A welding method for two members adapted to be welded and formed of a low-alloy steel for structural purposes causing the weld metal to develop martensite transformation during cooling after welding, so that the weld metal becomes expanded to a greater degree at room temperature than at a temperature at which the martensite transformation initiates. The welding material comprises a ferrous alloy containing C, Cr, Ni, Si, Mn, Mo and Nb, all of which meet substantially with the contents of the following equation (1): 170 ≤ 719 - (795 x C wt%) - (23.7 x Cr wt%) - (26.5 x Ni wt%) - (35.55 x Si wt%) - (13.25 x Mn wt%) - (23.7 x Mo wt%) - (11.85 x Nb wt%)
摘要:
In the present invention, an iron based alloy which contains by mass%; 0.20% or less of C; 6.0 to 16.0% of Cr; 6.0 to 16.0% of Ni and whose martensitic transformation starting temperature (Ms point temperature) is in the range of 0-170°C, inclusive of 0°C and exclusive of 170°C, is used as a welding material. With respect to a weld metal, the weld metal has a iron alloy composition which contains by mass%: 0.20% or less of C; 3.0 to 13.0% of Cr; 3.0 to 13.0% of Ni and whose martensitic transformation starting temperature (Ms point temperature) is in the range of 50-360°C, inclusive of both 50°C and 360°C.
摘要:
In the present invention, an iron based alloy which contains by mass%; 0.20% or less of C; 6.0 to 16.0% of Cr; 6.0 to 16.0% of Ni and whose martensitic transformation starting temperature (Ms point temperature) is in the range of 0-170°C, inclusive of 0°C and exclusive of 170°C, is used as a welding material. With respect to a weld metal, the weld metal has a iron alloy composition which contains by mass%: 0.20% or less of C; 3.0 to 13.0% of Cr; 3.0 to 13.0% of Ni and whose martensitic transformation starting temperature (Ms point temperature) is in the range of 50-360°C, inclusive of both 50°C and 360°C.