Light-sensitive silver halide photographic material having superior sharpness and feasible for ultra-rapid processing
    1.
    发明公开
    Light-sensitive silver halide photographic material having superior sharpness and feasible for ultra-rapid processing 失效
    具有超敏感敏感性和易于超快处理的感光银色摄影材料

    公开(公告)号:EP0307867A3

    公开(公告)日:1990-08-08

    申请号:EP88114957.9

    申请日:1988-09-13

    IPC分类号: G03C1/84 G03C5/16

    CPC分类号: G03C1/825 G03C5/16

    摘要: A light-sensitive silver halide photographic material comprising a support and, provided thereon, photographic component layers containing a gelatin and including a silver halide emulsion layer and a layer containing a dye, said dye having, as an aqueous solution, at least one maximum absorption wavelength (λ max ) in the range of from 400 nm to 850 nm, and the amount of gelatin present on the same side of said silver halide emulsion layer being within the range from 2.0 g/m² to 3.5 g/m² and a method of processing a imagewise exposed light-sensitive silver halide photographic material as above by the use of an automatic processing machine at a speed of 20 to 60 seconds.

    Silver halide photographic light-sensitive material capable of super-rapid processing
    2.
    发明公开
    Silver halide photographic light-sensitive material capable of super-rapid processing 失效
    超快速加工的银色摄影感光材料

    公开(公告)号:EP0267019A3

    公开(公告)日:1989-07-19

    申请号:EP87309756.2

    申请日:1987-11-04

    IPC分类号: G03C1/46 G03C1/38 G03C1/74

    摘要: A silver halide photographic light-sensitive material comprising a support having the first photographic structual layer comprising one or more layers on a side of the support and the second photographic structual layer comprising one or more layers on the other side of the support, in which at least one of the photographic structual layers comprises a silver halide light-sensitive emulsion layer, and the total amount of gelatin contained in the photographic structual layer comprising the silver halide emulsion layer is within the range of from 2.00 g/m² to 3.50 g/m². The uppermost layer of the photographic structual layer comprising the silver halide emulsion is formed by coating of a solution having a surface tention of from 15 to 26 dyn/cm, and the second photographic stuructual layer is coated and gelled between coating and drying of the first photographic structual layer. The photographic material is improved in the adaptability for super-rapid processing with the total duration of 20 to 60 sec. and the unti-scratch property.

    High-speed processing of silver halide photographic light- sensitive materials
    4.
    发明公开
    High-speed processing of silver halide photographic light- sensitive materials 失效
    Silchhalogenidmaterialen的Hochgeschwindigkeitsverarbeitung von photographisches lichtempfindliches。

    公开(公告)号:EP0282302A2

    公开(公告)日:1988-09-14

    申请号:EP88302089.3

    申请日:1988-03-10

    IPC分类号: G03C1/005 G03C5/29

    摘要: A silver halide photographic material which is capable of super-rapid processing with the total time of 20 to 60 minutes while processing high sensitivity, low fog and excellent pressure resistance and lack of graininess is described. The photographic material comprises a support bearing a hydrophilic colloidal layer including at least one light sensitive silver halide emulsion layer thereon, wherein at least some of the silver halide grains present in the said silver halide emulsion layer are tabular grains which have an aspect ratio of the grain size to the grain thickness of at least 5, such that the projective areas of said tabular grains represent not less than 50% of the projective areas of all the silver halide grains in said emulsion layer, the melting time taken for at least one silver halide emulsion layer of a 1 cm x 2 cm position of said silver halide photographic light-sensitive material in a 1.5% by weight aqueous solution of sodium hydroxide at 50°C to commence to dissolve is at least 45 minutes, and on the side bearing the hydrophilic colloidal layer containing said silver halide emulsion layer, gelatin is present in an amount from 2.00 to 3.20 g/m².

    摘要翻译: 描述了一种卤化银照相材料,其能够在加工高灵敏度,低雾和优异的耐压性和缺乏颗粒性的同时,总共20-60分钟的超快速处理。 所述照相材料包含支撑物,所述支持物具有包含至少一个感光卤化银乳剂层的亲水性胶体层,其中存在于所述卤化银乳剂层中的至少一些卤化银颗粒是片状颗粒,其具有 晶粒尺寸至晶粒厚度至少为5,使得所述片状颗粒的投影面积不小于所述乳剂层中所有卤化银颗粒的投影面积的50%,至少一种银的熔化时间 卤化银乳剂层中的卤化银摄影感光材料的1cm×2cm位置在1.5重量%氢氧化钠水溶液中于50℃开始溶解至少45分钟,而在侧面承载 含有所述卤化银乳剂层的亲水胶体层,明胶的存在量为2.00-3.20g / m 2。

    Light-sensitive silver halide photographic material having superior sharpness and feasible for ultra-rapid processing
    6.
    发明公开
    Light-sensitive silver halide photographic material having superior sharpness and feasible for ultra-rapid processing 失效
    感光卤化银照相材料具有优良的清晰度和适合于超快速的处理。

    公开(公告)号:EP0307867A2

    公开(公告)日:1989-03-22

    申请号:EP88114957.9

    申请日:1988-09-13

    IPC分类号: G03C1/84 G03C5/16

    CPC分类号: G03C1/825 G03C5/16

    摘要: A light-sensitive silver halide photographic material comprising a support and, provided thereon, photographic component layers containing a gelatin and including a silver halide emulsion layer and a layer containing a dye, said dye having, as an aqueous solution, at least one maximum absorption wavelength (λ max ) in the range of from 400 nm to 850 nm, and the amount of gelatin present on the same side of said silver halide emulsion layer being within the range from 2.0 g/m² to 3.5 g/m² and a method of processing a imagewise exposed light-sensitive silver halide photographic material as above by the use of an automatic processing machine at a speed of 20 to 60 seconds.

    摘要翻译: 光敏感的卤化银照相材料,其包含支承体和,设置在其上,将含有明胶和包含卤化银乳剂层和含染料的层,照相组成层所说的染料,如在wässrige溶液,至少一个最大吸收 波长(λ最大值)在从400nm至850nm的范围内,并且本明胶的在所述的卤化银乳剂层的同一侧的范围内为2.0克/米<2>至3.5克/米<量 2>和处理成像曝光感光卤化银照相材料如上述通过在20至60秒的速度使用自动加工机的方法。

    High-speed processing silver halide photographic lightsensitive material
    9.
    发明公开
    High-speed processing silver halide photographic lightsensitive material 失效
    高速加工银色摄影照明材料

    公开(公告)号:EP0282302A3

    公开(公告)日:1988-11-30

    申请号:EP88302089

    申请日:1988-03-10

    IPC分类号: G03C01/02

    摘要: A silver halide photographic material which is capable of super-rapid processing with the total time of 20 to 60 minutes while processing high sensitivity, low fog and excellent pressure resistance and lack of graininess is described. The photographic material comprises a support bearing a hydrophilic colloidal layer including at least one light sensitive silver halide emulsion layer thereon, wherein at least some of the silver halide grains present in the said silver halide emulsion layer are tabular grains which have an aspect ratio of the grain size to the grain thickness of at least 5, such that the projective areas of said tabular grains represent not less than 50% of the projective areas of all the silver halide grains in said emulsion layer, the melting time taken for at least one silver halide emulsion layer of a 1 cm x 2 cm position of said silver halide photographic light-sensitive material in a 1.5% by weight aqueous solution of sodium hydroxide at 50°C to commence to dissolve is at least 45 minutes, and on the side bearing the hydrophilic colloidal layer containing said silver halide emulsion layer, gelatin is present in an amount from 2.00 to 3.20 g/m².