摘要:
Disclosed is an aramid product in which the number of defects present in noncrystalline regions is considerably reduced and a composition for aramid for producing the same. The composition contains aromatic polyamide and a fused aromatic compound, wherein the content of the fused aromatic compound is 0.01 to 10 parts by weight, based on 100 parts by weight of the aromatic polyamide.
摘要:
Disclosed are an aramid composite which satisfies bulletproof performance required for the related art, is lightweight and exhibits superior adhesive strength, and a method for producing the same. The aramid composite includes an aramid fabric, an adhesive layer and a metal substrate, wherein at least one of the surface of the aramid fabric and the surface of the metal substrate is modified.
摘要:
The present invention provides a method for manufacturing para-aramid fibers, which includes: spinning a polymeric solution containing aramid polymer in an organic solvent through a spinneret into an inert gas to partially remove the organic solvent contained in the spun fiber; contacting the spun fiber with conditioning solution, so as to maintain residual water in fiber in a range of 10 to 15%; and subjecting the treated fiber to drawing, washing and heating in a dry-spinning manner. The present invention may greatly reduce energy consumption and costs for recovery of the solvent, as compared to a conventional manufacturing method of aramid fiber in a wet-spinning manner. Further, the present invention may solve conventional problems such as corrosion of apparatus, deterioration of working environments, or the like, since a concentrated sulfuric acid solvent is not used in a spinning process. Still further, the present invention may conduct drawing and heating after maintaining the residual water in fiber in a range of 10 to 15% before drawing, thereby remarkably improving the strength and elastic modulus of the fiber.
摘要:
The present invention provides a method for manufacturing para-aramid fibers, which includes: spinning a polymeric solution containing aramid polymer in an organic solvent through a spinneret into an inert gas to partially remove the organic solvent contained in the spun fiber; contacting the spun fiber with conditioning solution, so as to maintain residual water in fiber in a range of 10 to 15%; and subjecting the treated fiber to drawing, washing and heating in a dry-spinning manner. The present invention may greatly reduce energy consumption and costs for recovery of the solvent, as compared to a conventional manufacturing method of aramid fiber in a wet-spinning manner. Further, the present invention may solve conventional problems such as corrosion of apparatus, deterioration of working environments, or the like, since a concentrated sulfuric acid solvent is not used in a spinning process. Still further, the present invention may conduct drawing and heating after maintaining the residual water in fiber in a range of 10 to 15% before drawing, thereby remarkably improving the strength and elastic modulus of the fiber.
摘要:
An aramid fiber and a method of producing the same is disclosed, which is capable of realizing high surface uniformity and improved tensile strength and elongation property, wherein the method comprises preparing an aromatic polyamide by polymerizing aromatic diamine with aromatic diacid halide; preparing a spinning dope by dissolving the aromatic polyamide in a solvent; and extruding the spinning dope through a spinneret, and sequentially passing the spinning dope through an air gap, a coagulation bath filled with a coagulation solution, and a co¬ agulation tube having a jet opening, connected with the bottom of the coagulation bath, to obtain a filament wherein a distance from the upper surface of the coagulation solution contained in the coagulation bath to the jet opening of the coagulation tube is within a range between 10 and 35mm.
摘要:
An aramid fiber and a method of producing the same is disclosed, which is capable of realizing high surface uniformity and improved tensile strength and elongation property, wherein the method comprises preparing an aromatic polyamide by polymerizing aromatic diamine with aromatic diacid halide; preparing a spinning dope by dissolving the aromatic polyamide in a solvent; and extruding the spinning dope through a spinneret, and sequentially passing the spinning dope through an air gap, a coagulation bath filled with a coagulation solution, and a co¬ agulation tube having a jet opening, connected with the bottom of the coagulation bath, to obtain a filament wherein a distance from the upper surface of the coagulation solution contained in the coagulation bath to the jet opening of the coagulation tube is within a range between 10 and 35mm.