STEEL SHEET FOR HEAT-SHRINK BAND AND METHOD OF MANUFACTURING IT
    2.
    发明公开
    STEEL SHEET FOR HEAT-SHRINK BAND AND METHOD OF MANUFACTURING IT 审中-公开
    VERFAHREN ZU DESSEN HERSTELLUNG的STAHLPLATTEFÜRWÄRMESCHRUMPFFÄHIGES

    公开(公告)号:EP1098010A4

    公开(公告)日:2003-08-06

    申请号:EP99922537

    申请日:1999-05-28

    申请人: NIPPON KOKAN KK

    摘要: A steel sheet for a heat-shrink band having a composition containing not more than 0.1% of C, not more than 0.1% of Si, 0.1 to 2% of Mn, not more than 0.15% of P, not more than 0.02% of S, not more than 0.08% of solAl, and not more than 0.005% of N, or a composition containing not more than 0.005% of C, not more than 0.1% of Si, 0.1 to 2% of Mn, not more than 0.15% of P, not more than 0.02% of S, not more than 0.08% of solAl, not more than 0.005% of N, 0.02 to 0.06% of Ti and 0.0003 to 0.005% of B, and having, after being shrink-fitted, a product of a magnetic permeability and a sheet thickness (mm) of not smaller than 350 in a magnetic field of 0.30e, the steel sheet implementing a color CRT with a sufficient magnetic shielding feature and a slight color misregistering.

    摘要翻译: 本发明的热收缩带钢基于重量百分比C:0.1%以下,Si:0.1%以下,Mn:0.1〜2%,P:0.15%以下,S:0.02% 以下,溶胶Al:0.08%以下,N:0.005%以下或C:0.005%以下,Si:0.1%以下,Mn:0.1〜2%,P:0.15%以下,S: 0.02%以下,溶胶Al:0.08%以下,N:0.005%以下,Ti:0.02〜0.06%,B:0.0003〜0.005%,其中磁场的磁导率在0.3Oe以上的磁导率在 热收缩处理和厚度(mm)至少为350°。通过钢板可以实现具有足够的磁屏蔽特性和较少颜色偏差的彩色CRT。