公开(公告)号:EP1740325A1
公开(公告)日:2007-01-10
申请号:EP05722362.0
申请日:2005-04-07
申请人: Newearth PTE LTD
CPC分类号: C04B35/6316 , B09B3/005 , B09C1/067 , C02F11/008 , C02F2101/20 , C04B33/1327 , C04B33/30 , C04B33/32 , C04B35/62605 , C04B35/6261 , C04B35/6263 , C04B35/62655 , C04B35/63 , C04B35/6313 , C04B2235/3217 , C04B2235/3218 , C04B2235/3427 , C04B2235/3463 , C04B2235/6562 , F23G5/006 , F23G5/02 , F23G5/085 , F23G7/00 , F23G2201/701 , F23G2201/702 , F23G2202/20 , F23G2209/12 , F23G2209/24 , F23G2209/30 , Y02P40/69
摘要: A method is provided for heavy metal stabilisation comprising: mixing waste, comprising heavy metals, with molecular sieve with the proviso that carbon-based molecular sieve is excluded, and clay; and vitrifying the mixture. In particular, a method comprising the steps of: preparing a pre-stabilised mixture by mixing waste, comprising heavy metals, with the molecular sieve, and optionally other chemicals; mixing the pre-stabilised mixture with clay; and vitrifying the obtained mixture is provided. It also provides a product comprising heavy metals that have been stabilised into the structure of the clay-based ceramic matrix, wherein the product is a vitrified product of a mixture of at least waste, comprising heavy metals, molecular sieve (with the proviso that carbon-based molecular sieve is excluded) and clay.