公开(公告)号:EP2370604B1
公开(公告)日:2018-11-14
申请号:EP09755899.3
申请日:2009-11-18
CPC分类号: C21D8/1211 , C21D6/008 , C21D8/1222 , C21D8/1255 , C21D8/1272 , C21D9/46 , C21D2201/05 , C22C38/001 , C22C38/008 , C22C38/02 , C22C38/04 , C22C38/16
摘要: A process for producing grain oriented magnetic sheets by subjecting a steel slab ≦̸100 mm, containing 2.5-3.5% si, to the following operations: optional first heating, to a temperature T1≦̸1250° C.; first rough hot-rolling at T2 between 900 and 1200° C., the reduction ratio (% Rid) being at least 80% in the absence of a subsequent heating or, in the presence of a subsequent heating to T3≦̸1300° C., at least 60% determined by % Rid=80−(T3−T2)/5; second finishing hot-rolling at T4