ZEOLITE CATALYST AND METHOD OF PREPARING AND USE OF ZEOLITE CATALYST
    1.
    发明公开
    ZEOLITE CATALYST AND METHOD OF PREPARING AND USE OF ZEOLITE CATALYST 审中-公开
    用于提供和使用沸石催化剂的沸石催化剂和方法

    公开(公告)号:EP1928809A2

    公开(公告)日:2008-06-11

    申请号:EP06800818.4

    申请日:2006-08-03

    IPC分类号: C07C15/067

    摘要: A zeolite catalyst is prepared by treating a zeolite with a phosphorus compound to form a phosphorus-treated zeolite. The phosphorus-treated zeolite is heated to a temperature of about 3000C or higher and combined with an inorganic oxide binder material to form a zeolite-binder mixture. The zeolite-binder mixture is heated to a temperature of about 4000C or higher to form a bound zeolite catalyst. The bound zeolite may exhibit at least two 31P MAS NMR peaks with maxima at from about 0 to about -55 ppm, with at least one peak having a maximum at from about -40 to about -50 ppm. Zeolites containing 10-oxygen ring pores that have been prepared in such a way may be used in aromatic . alkylation by contacting the bound zeolite catalyst with an aromatic alkylation feed of an aromatic compound and an alkylating agent under reaction conditions suitable for aromatic alkylation.

    BOUND PHOSPHORUS-MODIFIED ZEOLITE CATALYST, METHOD OF PREPARING AND METHOD OF USING THEREOF
    2.
    发明公开
    BOUND PHOSPHORUS-MODIFIED ZEOLITE CATALYST, METHOD OF PREPARING AND METHOD OF USING THEREOF 审中-公开
    粘结的磷改性的沸石催化剂,工艺用于生产和使用方法

    公开(公告)号:EP1973653A2

    公开(公告)日:2008-10-01

    申请号:EP06848106.8

    申请日:2006-12-22

    IPC分类号: B01J29/04 B01J29/06 B01J29/00

    摘要: Disclosed is a bound phosphorus-modified zeolite catalyst. Zeolite is treated with a phosphorus compound to form the phosphorus-treated zeolite. Binder material is treated with a mineral acid prior to being bound with the phosphorus-modified zeolite. The binder material includes inorganic oxide materials, such as alumina, clay, aluminum phosphate and silica- alumina, in particular, a binder of alumina or clay or their combinations. The mineral acid includes hydrochloric acid, nitric acid, phosphoric acid or sulfuric acid. The phosphorus- treated zeolite is combined with the acid-treated inorganic oxide binder material to form a zeolite-binder mixture. Water is added to form an extrudable paste which maybe shaped and is heated to a temperature of about 4000C or higher to form a bound phosphorus-modified zeolite catalyst. For aromatic alkylation, the bound phosphorus-modified zeolite catalyst is contacted with an aromatic alkylation feed of an aromatic compound and an alkylating agent under reaction conditions suitable for aromatic alkylation.