摘要:
The invention relates to a casting material for producing casting molds for casting high-melting point materials. Said casting material comprises a powdered component that contains magnesium oxide and aluminum oxide, and a liquid component. The powdered component additionally contains a calcium aluminate and an alkali fluoride or alkaline-earth fluoride, and the liquid component contains a polyelectrolyte and an alkaline component, said alkaline component adjusting the pH of the liquid component at between 10 and 14. The powdered and the liquid component are mixed, a flowable slip is produced, which is used, once dried, solidified and sintered, to produce a hollow mold.
摘要:
The invention relates to the area of ceramics and to a ceramic flat membrane which is configured as a multi-channel element. The aim of the invention is to provide a ceramic flat membrane with a larger effective membrane surface. To this end, the inventive ceramic flat membrane consists of at least two layers of at least two sub-layers of different porosity, at least one of these layers having a non-planar geometry. The two layers are joined to each other with at least spot joins and integral joins. The invention also provides a method for producing a flat membrane of this type. According to this method, suspensions are produced from at least two ceramic powders of different particle size. Two sub-layers are formed from said suspensions, then dried and joined to form one layer. At least one layer which is embossed and sintered or unsintered is joined to a non-embossed, similarly embossed, differently embossed or differently structured, sintered or unsintered layer with at least spot joins and integral joins to form a flat membrane.
摘要:
The invention relates to a casting material for producing casting molds for casting high-melting point materials. Said casting material comprises a powdered component that contains magnesium oxide and aluminum oxide, and a liquid component. The powdered component additionally contains a calcium aluminate and an alkali fluoride or alkaline-earth fluoride, and the liquid component contains a polyelectrolyte and an alkaline component, said alkaline component adjusting the pH of the liquid component at between 10 and 14. The powdered and the liquid component are mixed, a flowable slip is produced, which is used, once dried, solidified and sintered, to produce a hollow mold.