摘要:
The invention relates to a method and a device for producing coloured glasses. The aim of the invention is to obtain a particularly intimate mixture and to enable a quick change of the melt at the same time. To this end, the following procedure steps are applied: a melt made of a compound or fragments of glass is produced, the glass melt is further processed in at least one additional vessel, the melt is supplied to a skull device (3) (skull pot or skull channel) during subsequent processing, a dye is supplied (6, 6.1) to the melt after the melt was in the melting station (1) but before the melt enters the skull device (3) or while said melt is in the skull device.
摘要:
The aim of the invention is to reduce the energy required for melting in a unit provided with cooled walls. According to the invention, a method is provided for melting inorganic materials in a skull crucible, wherein the temperature of at least one area of the melt is selected in such a way that it ranges from Teff -20 % to Teff +20 %. The temperature Teff is defined by the temperature at which energy consumption per weight unit of melt is at a minimum. The through-put rate is selected in such a way that it is adapted to the required residence time.
摘要:
The invention relates to a device for continuously melting and refining inorganic compounds, especially fragments of glass or batches. The inventive device comprises a melting pot (1) and a refining pot (3). An induction coil (5) is allocated to the refining pot (3), serves for coupling high-frequency energy into the content of the pot and surrounds the wall of the refining pot. The inventive device also comprises a connection line (2) which serves for conveying the melt from the melting pot (1) into the refining pot (3). According to the invention, the connection line (2) exits the melting pot (1) in the bottom area (1.1) thereof and enters the melting pot in the bottom area (3.1) of the refining pot (3).
摘要:
The aim of the invention is to reduce the energy required for melting in a unit provided with cooled walls. According to the invention, a method is provided for melting inorganic materials in a skull crucible, wherein the temperature of at least one area of the melt is selected in such a way that it ranges from Teff -20 % to Teff +20 %. The temperature Teff is defined by the temperature at which energy consumption per weight unit of melt is at a minimum. The through-put rate is selected in such a way that it is adapted to the required residence time.